검색결과 : 14건
No. | Article |
---|---|
1 |
Interpreting slip transmission through mechanically induced interface energies: a Fe-3%Si case study Aifantis KE, Deng H, Shibata H, Tsurekawa S, Lejcek P, Hackney SA Journal of Materials Science, 54(2), 1831, 2019 |
2 |
A multiphysics model that can capture crack patterns in Si thin films based on their microstructure Rethore J, Zheng H, Li H, Li JJ, Aifantis KE Journal of Power Sources, 400, 383, 2018 |
3 |
A computation study on the interplay between surface morphology and electrochemical performance of patterned thin film electrodes for Li-ion batteries Gur S, Frantziskonis GN, Aifantis KE Journal of Power Sources, 360, 504, 2017 |
4 |
Si micropyramid patterned anodes that can suppress fracture and solid electrolyte interface formation during electrochemical cycling Deng HK, Chu G, Luo F, Li H, Chen LQ, Aifantis KE Journal of Power Sources, 329, 372, 2016 |
5 |
Mechanical plasticity of cells Bonakdar N, Gerum R, Kuhn M, Sporrer M, Lippert A, Schneider W, Aifantis KE, Fabry B Nature Materials, 15(10), 1090, 2016 |
6 |
Measuring the Surface and Bulk Modulus of Polished Polymers with AFM and Nanoindentation Hoffman D, Miskioglu I, Aifantis KE, Drelich J Journal of Adhesion Science and Technology, 26(8-9), 1201, 2012 |
7 |
Capacity fade in Sn-C nanopowder anodes due to fracture Aifantis KE, Huang T, Hackney SA, Sarakonsri T, Yu AS Journal of Power Sources, 197, 246, 2012 |
8 |
Investigation of crack patterns and cyclic performance of Ti-Si nanocomposite thin film anodes for lithium ion batteries Wang YH, He Y, Xiao RJ, Li H, Aifantis KE, Huang XJ Journal of Power Sources, 202, 236, 2012 |
9 |
The influence of particle size and spacing on the fragmentation of nanocomposite anodes for Li batteries Dimitrijevic BJ, Aifantis KE, Hackl K Journal of Power Sources, 206, 343, 2012 |
10 |
Mechanical stability for nanostructured Sn- and Si-based anodes Aifantis KE, Hackney SA Journal of Power Sources, 196(4), 2122, 2011 |