검색결과 : 2건
No. | Article |
---|---|
1 |
Delayed Failure of Hi-Nicalon and Hi-Nicalon S Multifilament Tows and Single Filaments at Intermediate Temperatures (500 degrees-800 degrees C) Gauthier W, Lamon J Journal of the American Ceramic Society, 92(3), 702, 2009 |
2 |
Oxidation of Silicon Carbide Fibers During Static Fatigue in Air at Intermediate Temperatures Gauthier W, Pailler F, Lamon J, Pailler R Journal of the American Ceramic Society, 92(9), 2067, 2009 |