검색결과 : 8건
No. | Article |
---|---|
1 |
Characterization of Na1.3Al0.3Zr1.7(PO4)(3) solid electrolyte ceramics by impedance spectroscopy Kazakevicius E, Kezionis A, Zukauskaite L, Barre M, Salkus T, Zalga A, Selskis A, Orliukas A Solid State Ionics, 271, 128, 2015 |
2 |
Broadband high frequency impedance spectrometer with working temperatures up to 1200 K Kezionis A, Kazakevicius E, Salkus T, Orliukas A Solid State Ionics, 188(1), 110, 2011 |
3 |
Plasma oxidation of bilayered Y/Zr films Pranevicius L, Milcius D, Pranevicius LL, Orliukas A, Dudonis J, Laukaitis G Solid State Ionics, 179(1-6), 104, 2008 |
4 |
Impedance spectra of Li1.3Sc0.15Y0.15Ti1.7(PO4)(3) solid electrolyte ceramics in a broad frequency range Kazakevicius E, Dindune A, Kanepe Z, Ronis J, Orliukas A, Kezionis A, Salkus T Solid State Ionics, 176(19-22), 1743, 2005 |
5 |
Synthesis, structure and peculiarities of ionic transport of Li1.6Mg0.3Ti1.7(PO4)(3) ceramics Orliukas A, Dindune A, Kanepe Z, Ronis J, Kazakevicius E, Kezionis A Solid State Ionics, 157(1-4), 177, 2003 |
6 |
Relaxation dispersion of ionic conductivity of BICOVOX Kezionis A, Bogusz W, Krok F, Dygas J, Orliukas A, Abrahams I, Gebicki W Solid State Ionics, 119(1-4), 145, 1999 |
7 |
Electric Properties of Nh4Sn2F5 Polycrystals in the Frequency-Range from 20 to 3.2-Center-Dot-10(10) Hz Murin I, Peceliunaite A, Kezionis A, Mizaras R, Orliukas A Solid State Ionics, 86-88, 247, 1996 |
8 |
The Relaxation Dispersion of the Ionic-Conductivity in Cubic Zirconias Orliukas A, Bohac P, Sasaki K, Gauckler LJ Solid State Ionics, 72, 35, 1994 |