87 - 90 |
Ink jet printing of PZT aqueous ceramic suspensions Windle J, Derby B |
91 - 92 |
Preparation and characterization of Bi2Sr2CaCu2O8+x thick films on Ag substrate by a sol-gel process Li ZC, Cao GH, Fang MH, Jiao ZK |
93 - 95 |
The role of blade sharpness in cutting instabilities of polyethylene terephthalate Meehan RR, Kumar J, Earl M, Svenson E, Burns SJ |
97 - 98 |
Titanium dioxide synthesis by sol gel methods and evaluation of their photocatalytic activity Robert D, Weber JV |
99 - 101 |
Ceramic deposition using an electromagnetic jet printer station Wright MJ, Evans JRG |
103 - 106 |
The effect of Ti on the reaction phases at the interface between a Ag filler and Si3N4 Dummler W, Weber S, Tete C, Scherrer S |
107 - 110 |
Relations between microstructures, fracture mechanism and fatigue properties in structural materials Tanaka M, Kayama A, Kato R |
111 - 113 |
The characteristics of the diffusion between the as-reaction-formed Ni3Al intermetallic compound and pure nickel for interfacial bonding Duszczyk J, Zhou J, Marvina L, Zhuang LZ |
115 - 117 |
Characterization of ZnS nanoparticles prepared by new route Xu JF, Ji W |
119 - 121 |
A comparative study of fretting wear debris on (Ti,Al)N-coatings produced by different ion plating techniques Huq MZ, de Wit E, Celis JP |
123 - 125 |
Laser ablation behavior of a granulated Si target Zhang YF, Tang YH, Lee CS, Wang N, Bello I, Lee ST |
127 - 129 |
The photoelectrochemistry of Nd3+-doped TiO2 nanocrystalline electrodes Wang YQ, Cheng HM, Hao YZ, Ma JM, Xu B, Li WH, Cai SM |
131 - 133 |
Analysis of initial debonding propagation in layered materials Liu YF, Kagawa Y, Yuuki R |
135 - 136 |
Tensile and acoustic emission studies on carbon-BMI composites: effect of toughening aid on ILSS of composites Park SJ, Lee JR |
137 - 139 |
Distribution of the strength of the filamentary Nb3Al compound Ochiai S, Sawada T, Nishino S, Sekino H, Hojo M, Yamada Y, Hayashi K, Ayai N, Koganeya M, Ono M |
141 - 143 |
Multicarbide formation direct from concentrate Welham NJ |
145 - 147 |
Mechanical damping effect of greases in instrumented impact testing Aranyi Z, Murguly T, Molnar S, Bezeredi A, Pukanszky B |
149 - 151 |
A new wear model Mukhopadhay AK, Chanda A |
153 - 155 |
Lattice relaxation in heavily In-doped CdTe films Castro-Rodriguez R, Zapata-Navarro A, Zapata-Torres M, Pena JL |
157 - 158 |
Interfacial defects in AlN/W cofired substrates Liang TX, Zhu JG, Wang Y, Li HD |
159 - 161 |
Preparation and properties of Fe-fiber-strengthened copper composite Zhao XB, Wu ZT, Yuan TZ |
163 - 165 |
Grain growth of BaTiO3 Park ET |
167 - 169 |
The role of surface finish in contact brazing Mohandas T, Murthy VSR, Dutta A, Mallesham P |
171 - 172 |
Effect of impurities on wetting of mullite by cordierite liquid Ebadzadeh T, Lee WE |