1519 - 1520 |
Effects of Small Compressive Stress on T-C for High T-C Bi1.6Pb0.35Sb0.05Sr2Ca2Cu3Ox Oguri K, Kubota K, Kato F, Zakouji T, Sasaki H, Nishi Y |
1521 - 1523 |
A Possible Role for Surface Packing Density in the Formation of (111)Texture in Solidified fcc Metals Li DY, Szpunar JA |
1524 - 1527 |
Single-Fiber Polyethylene Epoxy Composites Young RJ, Gonzalezchi PI |
1528 - 1529 |
Solid Solubility of Chromium in Aluminum at 0.1-MPa and 2.1-GPa Yamane T, Kang YS, Miyamoto Y, Araki H, Minamino Y |
1530 - 1532 |
Effect of TiC Addition on the Microstructure and Properties of Ti(C,N)-WC-Co-Ni Cermet Laoui T, Vanderbiest O |
1533 - 1534 |
Oh-Related Capacitance-Voltage Recovery Effect in MOS Capacitors Passivated by ZnO-B2O3-P2O5-SiO2 Glasses .4. The Effects of BaO Content Kobayashi K |
1535 - 1537 |
A Preliminary Nuclear-Magnetic-Resonance Investigation of the Titanium Diisopropoxide bis(2,4-Pentanedionate) Propanediol Sol-Gel Precursor System Phillips NJ, Milne SJ, Ali NJ, Kennedy JD |
1538 - 1539 |
Synthesis and Application of Hybrid Organic-Inorganic Colloidal Gels Ayral A, Guizard C, Cot L |
1540 - 1542 |
Catalytic Profiles of Palladium Clusters on Zeolite in Reduction of Nitrogen Monoxide with Propane Tanabe S, Matsumoto H |
1543 - 1545 |
Solid-State Chemistry of Alumina-Chromia-Magnesia and Related Refractories Aldouri WA, Davies TJ, Ogwu AA, Emblem HG |
1546 - 1550 |
Investigation of the Influence of Machining on the Fracture of Engineering Ceramics Shemilt JE, Siddiqui AA, Bradwell SC |
1551 - 1554 |
Scanning Electron-Acoustic Microscopy Imaging of Subsurface Microcracks Produced in Gear Fatigue Shaw BA, Evans JT, Page TF |
1555 - 1557 |
Some Considerations on the 2nd-Phase Structure in High-Impact Polystyrene and on the Related Measurement Methods Anzaldi S, Bonifaci L, Malaguti E, Vighi M, Ravanetti GP |
1558 - 1560 |
Effect of X-Ray-Irradiation on Dielectric-Properties of ZnF2-PbO-TeO2 Glasses Kumar VR, Veeraiah N, Murthy JS |
1561 - 1563 |
Improvement of Superplastic Properties of Ti-6Al-4V Alloy by Temporary Alloying with Hydrogen Gong B, Zhang CB, Lai ZH |
1564 - 1566 |
Zirconia-13 Mol-Percent Calcia Solid-Solution Synthesis by the Polymerized Complex and Coprecipitation Routes Yashima M, Ohtake K, Kakihana M, Yoshimura M |
1567 - 1569 |
Surface Reduction of Iron-Chromium-Molybdenum Oxide Catalysts for Methanol Oxidation Pesheva Y, Nemska S, Stefanov P, Klissurski D, Rives V |
1570 - 1572 |
Photoluminescence of Se-Annealed CuInSe2 Powders Krustok J, Madasson J, Hjelt K |
1573 - 1576 |
Effects of Galvanostatic Treatments on Hot Corrosion of Ni Kim JJ, Cho SM |
1577 - 1578 |
A Quantitative-Analysis of the Size of the Kanzig Regions Ganesh R, Goo E |
1579 - 1581 |
Preparation of Stable, High-Surface-Area Zirconia Chan KS, Chuah GK, Jaenicke S |
1582 - 1584 |
Crystal-Growth of Bi2Sr2Cacu2O8 Superconductors by a Self-Flux Method Roy SN, Devi PS, Basu RN, Maiti HS |
1585 - 1587 |
The Angular-Distribution of Sputtered Atoms and the Influence of Topographic Features Wang ZX, Pan JS, Zhang JP, Tao ZL |
1588 - 1590 |
Phase-Transition and Particulate Growth of Laser Synthesized Ultrafine Amorphous-Silicon Nitride Powders Li Y, Liang Y, Zheng F, Shong X, Hu Z |
1591 - 1593 |
Sputtering and Roughness of the (001)Copper, (011)Copper and (111)Copper Single-Crystal Planes Moreno D, Eliezer D |