6983 - 6987 |
A fuel cell operating between room temperature and 250 degrees C based on a new phosphoric acid based composite electrolyte Lan R, Xu XX, Tao SW, Irvine JTS |
6988 - 6996 |
Degradation mechanism of molten carbonate fuel cell based on long-term performance: Long-term operation by using bench-scale cell and post-test analysis of the cell Morita H, Kawase M, Mugikura Y, Asano K |
6997 - 7002 |
Microstructural evolution of ball-milled MgH2 during a complete dehydrogenation-hydrogenation cycle Revesz A, Fatay D |
7003 - 7010 |
Phase change in the cathode side of a proton exchange membrane fuel cell Khajeh-Hosseini-Dalasm N, Fushinobu K, Okazaki K |
7011 - 7024 |
Mass transport analysis of a passive vapor-feed direct methanol fuel cell Xu C, Faghri A |
7025 - 7032 |
Hydrogen sulfide poisoning in solid oxide fuel cells under accelerated testing conditions Li TSA, Wang WG, Chen T, Miao H, Xu C |
7033 - 7037 |
Reversible poisoning of nickel/zirconia solid oxide fuel cell anodes by hydrogen chloride in coal gas Marina OA, Pederson LR, Thomsen EC, Coyle CA, Yoon KJ |
7038 - 7041 |
BaZr0.1Ce0.7Y0.1Yb0.1O3-delta electrolyte-based solid oxide fuel cells with cobalt-free PrBaFe2O5+delta layered perovskite cathode Ding HP, Xue XJ |
7042 - 7045 |
A cobalt-free SrFe0.9Sb0.1O3-delta cathode material for proton-conducting solid oxide fuel cells with stable BaZr0.1Ce0.7Y0.1Yb0.1O3-delta electrolyte Ling YH, Zhang XZ, Wang SL, Zhao L, Lin B, Liu XQ |
7046 - 7053 |
Fabrication of solid oxide fuel cell anode electrode by spray pyrolysis Liu L, Kim GY, Chandra A |
7054 - 7060 |
Layer by layer assembly of hybrid nanoparticle coatings for proton exchange membrane fuel cell bipolar plates Wang F, Alazemi M, Dutta I, Blunk RH, Angelopoulos AP |
7061 - 7066 |
Performance of a proton exchange membrane fuel cell stack using conductive amorphous carbon-coated 304 stainless steel bipolar plates Yi PY, Peng LF, Feng LZ, Gan P, Lai XM |
7067 - 7077 |
Modeling, simulation and optimization of a no-chamber solid oxide fuel cell operated with a flat-flame burner Vogler M, Horiuchi M, Bessler WG |
7078 - 7082 |
Fabrication of catalyst-coated membrane-electrode assemblies by doctor blade method and their performance in fuel cells Park IS, Li W, Manthiram A |
7083 - 7089 |
Microwave assisted synthesis of surfactant stabilized platinum/carbon nanotube electrocatalysts for direct methanol fuel cell applications Sakthivel M, Schlange A, Kunz U, Turek T |
7090 - 7097 |
Low-temperature behavior of graphite-tin composite anodes for Li-ion batteries Nobili F, Mancini M, Dsoke S, Tossici R, Marassi R |
7098 - 7101 |
Synthesis of single crystalline Li0.44MnO2 nanowires with large specific capacity and good high current density property for a positive electrode of Li ion battery Hosono E, Matsuda H, Saito T, Kudo T, Ichihara M, Honma I, Zhou HS |
7102 - 7114 |
One-dimensional dynamic modeling and validation of maintenance-free lead-acid batteries emphasizing temperature effects Siniard K, Xiao M, Choe SY |
7115 - 7119 |
Effect and function mechanism of amorphous sulfur on the electrochemical properties of cobalt hydroxide electrode Song DW, Wang YJ, Wang QH, Wang YP, Jiao LF, Yuan HT |
7120 - 7125 |
Symmetric redox supercapacitor based on micro-fabrication with three-dimensional polypyrrole electrodes Sun W, Zheng RL, Chen XY |
7126 - 7127 |
Elevated temperature cycling stability and electrochemical impedance of LiMn2O4 cathodes with nanoporous ZrO2 and TiO2 coatings (vol 195, pg 4943, 2010) Walz KA, Johnson CS, Genthe J, Stoiber LC, Zeltner WA, Anderson MA, Thackeray MM |