1077 - 1098 |
Local phenomena in oxides by advanced scanning probe microscopy Kalinin SV, Shao R, Bonnell DA |
1099 - 1107 |
Stability of mullite protective coatings for silicon-based ceramics Krishnamurthy R, Sheldon BW, Haynes JA |
1108 - 1114 |
Porous ceramic bodies with interconnected pore channels by a novel freeze casting technique Araki K, Halloran JW |
1115 - 1121 |
Effect of liquid phase sintering on microstructure and mechanical properties of Yb2O3-AlN containing SiC-based ceramics Izhevskyi VA, Bressiani AHA, Bressiani JC |
1122 - 1126 |
Fixing arsenic in alkali-activated cementitious matrices Fernandez-Jimenez A, Palomo A, Macphee DE, Lachowski EE |
1127 - 1132 |
Deterministic microgrinding, lapping, and polishing of glass-ceramics Lambropoulos JC, Jacobs SD, Gillman BE, Stevens HJ |
1133 - 1138 |
Aqueous synthesis at 200 degrees C of sub-10 nanometer yttria tetragonally stabilized zirconia using a metal-ligand approach Kimel RA, Adair JH |
1139 - 1144 |
Oxidation of silicon nitride in wet air and effect of lutetium disilicate coating Suetsuna T, Ohji T |
1145 - 1149 |
Influence of surface cleaning and calcination on rheological properties of silicon carbide aqueous suspensions Li W, Cheng P, Gu MY |
1150 - 1157 |
Zirconia-mullite composites consolidated by spark plasma reaction sintering from zircon and alumina Rocha-Rangel E, Diaz-de-la-Torre S, Umemoto M, Miyamoto H, Balmori-Ramirez H |
1158 - 1164 |
Ceramic composites with three-dimensional architectures designed to produce a threshold strength - 1. Processing Fair GE, Lange FF |
1165 - 1170 |
Camber development during the cofiring of bi-layer glass-based dielectric laminate Chang JC, Jean JH |
1171 - 1174 |
Vacuum-assisted microfluidic lithography of ceramic microstructures Ahn SJ, Moon J |
1175 - 1179 |
Sol-gel synthesis and characterization of alumina-calcium hexaaluminate composites Vishista K, Gnanam FD, Awaji H |
1180 - 1185 |
Structure evolution of an NiO-YSZ electrocatalytic electrode Aronin A, Abrosimova G, Bredikhin S, Matsuda K, Maeda K, Awano M |
1186 - 1189 |
The optical properties and band gap energy of nanocrystalline La0.4Sr0.6TiO3 thin films Suzuki T, Jasinski P, Petrovsky V, Anderson HU |
1190 - 1196 |
Processing and piezoelectric properties of lead-free (K,Na) (Nb,Ta) O-3 ceramics Matsubara M, Yamaguchi T, Sakamoto W, Kikuta K, Yogo T, Hirano S |
1197 - 1200 |
Effect of stacking layers on the microwave dielectric properties of MgTiO3/CaTiO3 multilayered thin films Lee BD, Lee HR, Yoon KH, Kang DH |
1201 - 1204 |
Preparation of single-phase high T-c superconductor (Bi,Pb)(2)Sr2Ca2Cu3Ox (2223) with Hg substitution Mackinnon CW, Li DY, Low IM |
1205 - 1208 |
Effects of the weak absorption tail on the transmission loss of Ge-Sb-Se optical fibers Chung WJ, Park BJ, Seo HS, Ahn JT, Lee MH, Choi YG |
1209 - 1212 |
Structural variation of the BaTi4O9 thin films grown by RF magnetron sputtering Jang BY, Jeong YH, Lee SJ, Lee KJ, Nahm S, Sun HJ, Lee HJ |
1213 - 1221 |
Thermal expansion kinetics: Method to measure permeability of cementitious materials, IV. Effect of thermal gradients and viscoelasticity Ciardullo JP, Sweeney DJ, Scherer GW |
1222 - 1226 |
Direct observations of debonding of reinforcing grains in silicon nitride ceramics sintered with yttria plus alumina additives Becher PF, Painter GS, Lance MJ, Ii S, Ikuhara Y |
1227 - 1232 |
Temperature-time-mechanical properties of glass-ceramics produced from coal fly ash Kim JM, Kim HS |
1233 - 1238 |
The mechanics of indentation induced lateral cracking Chen X, Hutchinson JW, Evans AG |
1239 - 1243 |
Friction and wear properties of Si3N4/carbon fiber composites with aligned microstructure Hyuga H, Jones MI, Hirao K, Yamauchi Y |
1244 - 1252 |
Structural behavior of oxygen permeable SrFe0.2Co0.8Ox ceramic membranes with and without pO(2) gradients Li YP, Maxey ER, Richardson JW |
1253 - 1260 |
Model apatite systems for the stabilization of toxic metals: II, cation and metalloid substitutions in chlorapatites Kim JY, Dong ZL, White TJ |
1261 - 1267 |
Atomic force microscopy study and qualitative analysis of martensite relief in zirconia Deville S, Chevalier J, El Attaoui H |
1268 - 1272 |
Ti2ZrO phases formed in the titanium and zirconia interface after reaction at 1550 degrees C Lin KL, Lin CC |
1273 - 1280 |
Microstructural investigation of the aging behavior of (3Y-TZP)-Al2O3 composites Deville S, Chevalier J, Dauvergne C, Fantozzi G, Bartolome JF, Moya JS, Torrecillas R |
1281 - 1289 |
Ionic-exchange mechanism in the formation of medieval luster decorations Pradell T, Molera J, Roque J, Vendrell-Saz M, Smith AD, Pantos E, Crespo D |
1290 - 1296 |
The 1300 degrees C isothermal section in the Ti-In-C ternary phase diagram Ganguly A, Barsoum MW, Schuster J |
1297 - 1301 |
Sintering additives to eliminate interphases in cordierite ceramics Shi ZM |
1302 - 1308 |
Microstructural evolution on firing soda-lime-silica glass fluxed whitewares Tarvornpanich T, Souza GP, Lee WE |
1309 - 1311 |
Biocomplatibility of fluor-hydroxyapatite bioceramics Lee EJ, Kim HW, Kim HE |
1312 - 1314 |
Characterization of chemical solution deposition-derived lead hafnate titanate thin films Schorn PJ, Schneller T, Bottger U, Waser R |
1315 - 1317 |
Crack bifurcation at the surface of laminar ceramics that exhibit a threshold strength Pontin MG, Lange FF |
1318 - 1320 |
Combustion reaction during mechanical alloying synthesis of Ti3SiC2 ceramics from 3Ti/Si/2C powder mixture Li JF, Matsuki T, Watanabe R |
1321 - 1322 |
Degradation of magnesium aluminum spinel by lithium fluoride sintering aid Villalobos GR, Sanghera JS, Aggarwal ID |
1323 - 1326 |
Influence of planetary high-energy ball milling on microstructure and mechanical properties of silicon nitride ceramics Liu XJ, Huang ZY, Pu XP, Sun XW, Huang LP |
1327 - 1330 |
Thermal performance of mechanically activated tetracalcium phosphate Gbureck U, Hofmann MP, Barralet JE |
1331 - 1333 |
Cyclic fatigue crack growth in PZT under mechanical loading Salz CRJ, Hoffman M, Westram I, Rodel J |
1334 - 1336 |
Fabrication of porous hydroxyapatite using hydrothermal hot pressing and post-sintering Nakahira A, Murakami T, Onoki T, Hashida T, Hosoi K |
1337 - 1340 |
Preparation of Ca3Co4O9 and improvement of its thermoelectric properties by spark plasma sintering Liu YH, Lin YH, Shi Z, Nan CW, Shen ZJ |
1341 - 1344 |
Aqueous synthesis of Y2O2S : Eu/silica core-shell particles Chung CC, Jean JH |
1345 - 1348 |
Compressibility and phase transition kinetics of lanthanide-doped zircon van Westrenen W, Frank MR, Fei YW, Fei YW, Hanchar JM, Finch RJ, Zha CS |
1349 - 1352 |
Low-temperature synthesis of nanosized bismuth ferrite by soft chemical route Ghosh S, Dasgupta S, Sen A, Maiti HS |
1353 - 1355 |
Reaction-formed porous Yb4Si2N2O7 materials with uniform open-cell network structure Zhu XW, Zhou Y, Hirao K |
1356 - 1358 |
Thermal expansion properties of lanthanum-substituted lead titanate ceramics Jun C, Xing XR, Yu RB, Liu GR |
1359 - 1361 |
Dry powder processing of fibrous fumed silica compacts for thermal insulation Abe HY, Abe I, Sato K, Naito M |
1362 - 1365 |
Effect of oxidation on crack deflection in SiC/Al2O3 laminated ceramic composites Krishnamurthy R, Rankin J, Sheldon BW |