1654 - 1680 |
Solid-state ionics: Roots, status, and future prospects Knauth P, Tuller HL |
1681 - 1688 |
Nonaqueous aluminum nitride extrusion: I, die-entry flow behavior Wight JF, Reed JS |
1689 - 1694 |
Nonaqueous aluminum nitride extrusion: II, die-land flow and tribology Wight JF, Reed JS |
1695 - 1698 |
Direct coagulation casting of alumina suspensions using Jack bean as a urease source Studart AR, Pandolfelli VC, Tervoort E, Gauckler LJ |
1699 - 1705 |
Rheology of cross-linked chitosan-alumina suspensions used for a new gelcasting process Johnson SB, Dunstan DE, Franks GV |
1706 - 1712 |
Densification of precursor-derived Si-C-N ceramics by high-pressure hot isostatic pressing Ishihara S, Gu H, Bill J, Aldinger F, Wakai F |
1713 - 1718 |
Bismuth oxide nanoparticles by flame spray pyrolysis Madler L, Pratsinis SE |
1719 - 1724 |
Formation of nanocrystalline transition-metal ferrites inside a silica matrix Rajic N, Ceh M, Gabrovsek R, Kaucic V |
1725 - 1729 |
Fabrication of transparent yttria ceramics by the low-temperature synthesis of yttrium hydroxide Ikegami T, Li JG, Mori T, Moriyoshi Y |
1730 - 1734 |
Use of mixed-rare-earth oxide in the preparation of reaction-bonded mullite at <= 1300 degrees C Kim HS, Nicholson PS |
1735 - 1737 |
Electrophoretic deposition of lead zirconate titanate ceramics Ma J, Cheng W |
1738 - 1744 |
Formation and properties of hydroxyapatite-calcium poly(vinyl phosphonate) composites Greish YE, Brown PW |
1745 - 1749 |
Comparative lattice-dynamical study of the Raman spectra of monoclinic and tetragonal phases of zirconia and hafnia Quintard PE, Barberis P, Mirgorodsky AP, Merle-Mejean T |
1750 - 1752 |
Direct formation of crystalline gadolinium-doped ceria powder via polymerized precursor solution Wang S, Maeda K |
1753 - 1756 |
Raman spectroscopic study of gallium-doped Ba(Zn1/3Ta2/3)O-3 Webb SJ, Breeze J, Scott RI, Cannell DS, Iddles DM, Alford NM |
1757 - 1762 |
Microstructure and grain-boundary effect on electrical properties of gadolinium-doped ceria Zhou XD, Huebner W, Kosacki I, Anderson HU |
1763 - 1769 |
Creep of duplex alumina-titanium nitride polycrystalline microstructures Tai Q, Mocellin A |
1770 - 1776 |
Characterization and tribological investigation of sol-gel titania and doped titania thin films Zhang WG, Liu WM, Li B, Mai GX |
1777 - 1782 |
Biaxial flexure strength and dynamic fatigue of soda-lime-silica float glass Krohn MH, Hellmann JR, Shelleman DL, Pantano CG, Sakoske GE |
1783 - 1787 |
Influence of surface residual stress state on crack path evolution in polycrystalline alumina Fang Y, Ravi-Chandar K, White KW |
1788 - 1792 |
Characteristics of a NaOH-Activated blast furnace slag blended with a fine particle silica waste Escalante-Garcia JI, Palacios-Villanueva VM, Gorokhovsky AV, Mendoza-Suarez G, Fuentes AF |
1793 - 1803 |
Model analysis of multicrack mechanisms in ceramic/superplastic laminates Deng ZY, Zhang GJ, Ando M, Ohji T |
1804 - 1806 |
Effect of substituent ions on martensitic transformation temperatures in dicalcium silicate solid solutions Fukuda K, Taguchi H, Fukuda T |
1807 - 1814 |
Thermal stability, phase evolution, and crystallization in Si-B-C-N ceramics derived from a polyborosilazane precursor Janakiraman N, Weinmann M, Schuhmacher J, Muller K, Bill J, Aldinger F, Singh P |
1815 - 1822 |
Developing interfacial carbon-boron-silicon coatings for silicon nitride-fiber-reinforced composites for improved oxidation resistance Sato K, Morozumi H, Funayama O, Kaya H, Isoda T |
1823 - 1826 |
Novel method for obtaining corundum layers of high surface area on ceramic supports for high-temperature catalysis Souto A, Guitian F |
1827 - 1834 |
Anomalous temperature dependence of the growth rate of the reaction layer between silica and molten aluminum Yoshikawa N, Kikuchi A, Taniguchi S |
1835 - 1840 |
Microstructural evolution in liquid-phase-sintered SiC: Part III, effect of nitrogen-gas sintering atmosphere Ortiz AL, Bhatia T, Padture NP, Pezzotti G |
1841 - 1844 |
Equilibrium shape of internal cavities in ruby and the effect of surface energy anisotropy on the equilibrium shape Choi JH, Kim DY, Hockey BJ, Wiederhorn SM, Blendell JE, Handwerker CA |
1845 - 1852 |
Original Monte Carlo methodology devoted to the study of sintering processes Bordere S |
1853 - 1859 |
Incorporation of uranium in zirconolite (CaZrTi2O7) Vance ER, Lumpkin GR, Carter ML, Cassidy DJ, Ball CJ, Day RA, Begg BD |
1860 - 1866 |
Oxidation of a silicon nitride-titanium nitride composite: Microstructural investigations and phenomenological modeling Deschaux-Beaume F, Cutard T, Frety N, Levaillant C |
1867 - 1869 |
Preparation and aging behavior of chemical-solution-deposited (Pb(Mg1/3Nb2/3)O-3)(1-x)(PbTiO3)(x) thin films without seeding layers Hoffmann M, Hofer C, Schneller T, Bottger U, Waser R |
1870 - 1872 |
Laser sintering of bismuth germanate (Bi4Ge3O12) ceramics Macedo ZS, Hernandes AC |
1873 - 1875 |
Resource recovery of waste incineration fly ash: Synthesis of zeolites A and P Miyake M, Tamura C, Matsuda M |
1876 - 1878 |
Experimental archaeology: Investigation on the copper-aluminum-silicon-oxygen system Woelk HJ, Hoffmann B, Mestl G, Schloegl R |
1879 - 1881 |
Synthesis and properties of porous single-phase beta'-SiAlON ceramics Yang JF, Beppu Y, Zhang GJ, Ohji T, Kanzaki S |
1882 - 1884 |
Effect of heating schedule on the microstructure and fracture toughness of alpha-SiAlON - Cause and solution Zenotchkine M, Shuba R, Chen IW |
1885 - 1887 |
Micropatterned ceramics by casting into polymer molds Schonholzer UP, Stutzmann N, Tervoort TA, Smith P, Gauckler LJ |
1888 - 1890 |
Photoluminescence probing of the formation of titanium dioxide sols from a titanium peroxide solution Seok SI, Kim MS, Suh TS |
1891 - 1893 |
Effect of 1600 degrees C heat treatment on C/SiC composites fabricated by polymer infiltration and pyrolysis with allylhydridopolycarbosilane Berbon M, Calabrese M |
1894 - 1896 |
Preparation of aluminum nitride-silicon carbide nanocomposite powder by the nitridation of aluminum silicon carbide Itatani K, Tsukamoto R, Delsing ACA, Hintzen HT, Okada I |
1897 - 1899 |
Growth of yttria-stabilized zirconia thin films on textured silver substrates by chemical vapor deposition Kim GS, Hwang SC, Kim YS, Shin HS |
1900 - 1902 |
High-strain-rate superplasticity inY(2)O(3)-stabilized tetragonal ZrO2 dispersed with 30 vol% MgAl2O4 spinel Morita K, Hiraga K, Sakka Y |
1903 - 1903 |
Comment on "high-temperature mechanical properties of Si-B-C-N-precursor-derived amorphous ceramics and the applicability of deformation models developed for metallic glasses" Khonik VA |