1 - 5 |
Preparation of TiO2 fibers by two-step synthesis method and their photocatalytic activity Zhang SY, Chen ZH, Li YL, Wang Q, Wan L, You Y |
6 - 8 |
A new route for obtaining Prussian blue nanoparticles Vo V, Van MN, Lee HI, Kim JM, Kim Y, Kim SJ |
9 - 12 |
Synthesis of hexagonal nanosized silver sulfide at room temperature Wang XB, Zhang SH, Zhang ZC |
13 - 17 |
Study on the growth mechanism of silver nanorods in the nanowire-seeding polyol process Chen C, Wang L, Yu HJ, Jiang GH, Yang Q, Zhou JF, Xiang WD, Zhang JF |
18 - 22 |
Dielectric properties of Mg-modified Pb(NbMo)O-3 system ceramics Singh NK, Rai R, Choudhary RNP |
23 - 27 |
Growth and characterization of an organometallic nonlinear optical material tri-allylthiourea cadmium chloride (ATCC) Perumal R, Babu SM |
28 - 32 |
Influence of solvent on the structural and morphological properties of AgI particles prepared using ultrasonic spray pyrolysis Validzic IL, Jokanovic V, Uskokovic DP, Nedeljkovic JM |
33 - 38 |
Optical and structural characterization of nickel oxide-based thin films obtained by chemical bath deposition Vidales-Hurtado MA, Mendoza-Galvan A |
39 - 43 |
Effect of composition and forming parameter on evaporated Ag-As-Te thin films Ei-Sayed SM, Saad HM |
44 - 50 |
The corrosion inhibition of mild steel by 3-formyl-8-hydroxy quinoline in hydrochloric acid medium Achary G, Sachin HR, Naik YA, Venkatesha TV |
51 - 56 |
Structural, thermal, mechanical and optical properties of L-arginine diiodate crystal: A new nonlinear optical material Sankar R, Muralidharan R, Raghavan CM, Jayavel R |
57 - 60 |
Growth and characterization of semiorganic nonlinear optical rubidium bis-DL-malato borate single crystals Balasubramanian D, Sankar R, Shankar VS, Murugakoothan P, Arulmozhichelvan P, Jayavel R |
61 - 66 |
Solidification of liquid electrolyte with imidazole polymers for quasi-solid-state dye-sensitized solar cells Wang M, Lin Y, Zhou XW, Xiao XR, Yang L, Feng SJ, Li XP |
67 - 71 |
Spark plasma sintering of alpha-Si3N4 ceramics with MgO-AlPO4 as sintering additives Chen F, Shen Q, Yan FQ, Zhang LM |
72 - 76 |
Leakage current behavior of Bi3.25La0.75Ti3O12 ferroelectric thin films deposited on different bottom electrodes Simoes AZ, Ramirez MA, Longo E, Varela JA |
77 - 81 |
Effect of urea on the photoactivity of titania powder prepared by sol-gel method Cheng P, Deng CS, Gu MY, Dai XM |
82 - 84 |
Photoluminescence of langasite thin films prepared from sol-gel process Hu Y, Wang FW, Lin HL |
85 - 90 |
Morphology-tunable synthesis and characterizations of Mg(OH)(2) films via a cathodic electrochemical process Zou GL, Chen WX, Liu R, Xu ZD |
91 - 95 |
Synthesis of highly ordered Iron/Cobalt nanowire arrays in AAO templates and their structural properties Luo ZX, Yan F, Zhou XF, Yao HN |
96 - 100 |
Effect of LiCl filler on the structure and morphology of PVDF films Elashmawi IS |
101 - 109 |
Redox properties of phenosafranine at zeolite-modified electrodes -Effect of surface modification and solution pH Easwaramoorthi S, Natarajan P |
110 - 114 |
Heating rate and temperature effects on the BaTiO3 formation by thermal decomposition of (Ba,Ti) organic precursors during the Pechini process Ramajo L, Parra R, Reboredo M, Zaghete M, Castro M |
115 - 121 |
Thermal-heating CVD synthesis of BN nanotubes from trimethyl borate and nitrogen gas Lin FH, Hsu CK, Tang TP, Kang PL, Yang FF |
122 - 126 |
Diameter-controlled growth of In2O3 nanowires on the surfaces of indium grains Dong HX, Yang HQ, Yang WY, Yin WY, Chen DC |
127 - 131 |
Structure and sensing properties of 0.1SnO(2)-0-9 alpha-Fe2O3 system Sorescu M, Diamandescu L, Tomescu A, Tarabasanu-Mihaila D, Teodorescu V |
132 - 136 |
Hydrothermal synthesis of stable mesoporous ZrO2-Y2O3 and CeO2-ZrO2-Y2O3 from simple inorganic salts and CTAB template in aqueous medium Feng RM, Yang XJ, Ji WJ, Au CT |
137 - 141 |
Rod-like zinc oxide constructed by nanoparticles: synthesis, characterization and optical properties Ha ZG, Yue LH, Zheng YF, Xu ZD |
142 - 147 |
Long lasting behavior of Gd2O2S : Eu3+ phosphor synthesized by hydrothermal routine Hang T, Liu Q, Mao DL, Chang CK |
148 - 152 |
Wear and corrosion resistant coatings formed by microarc oxidation on TiAl alloy Li XJ, Cheng GA, Xue WB, Zheng RT, Cheng YJ |
153 - 157 |
Evaluating two new synthesized S-N Schiff bases on the corrosion of copper in 15% hydrochloric acid Behpour M, Ghoreishi SM, Salavati-Niasari M, Ebrahimi B |
158 - 163 |
Interaction of TC4 titanium alloy with NiCrAlY coating after vacuum heat treatment Peng XM, Xia CQ, Ma K, Dai XY |
164 - 170 |
Adhesion force behavior between two gels attached with an electrolytic polymer liquid Tamagawa H, Takahashi Y |
171 - 176 |
Synthesis and characterization of LiNi1-xCoxO2 for lithium batteries by a novel method Li DC, Peng ZH, Ren HB, Guo WY, Zhou YH |
177 - 182 |
Electroluminescence of ZnO nanocrystalline particles annealed from mesoporous precursors Li J, Zhao XP, Yan CM, Luo YJ |