203 - 204 |
Nanocomposites of Sn and Li2O formed from the chemical reduction of SnO as negative electrode material for lithium-ion batteries Foster DL, Wolfenstine J, Read JR, Behl WK |
205 - 208 |
Amorphous ruthenium-chromium oxides for electrochemical capacitors Jeong YU, Manthiram A |
209 - 212 |
Nonaqueous phase Fe(VI) electrochemical storage and discharge of super-iron/lithium primary batteries Licht S, Wang BH |
213 - 215 |
Networks of electron-conducting polymer in matrices of ion-conducting polymers - Applications to fast electrodes Ghosh S, Inganas O |
216 - 219 |
Lithium depth profile in NiO molten carbonate fuel cell cathode by nuclear microprobe Belhomme C, Cassir M, Tessier C, Berthoumieux E |
220 - 223 |
In situ photoelectron spectroscopy study of a TiS2 cathode in an operating battery system Tonti D, Pettenkofer C, Jaegermann W |
224 - 227 |
Voltammetry at boron-doped diamond electrodes in liquid ammonia: Solvent window effects and diamond surface modification Del Campo FJ, Goeting CH, Morris D, Foord JS, Neudeck A, Compton RG, Marken F |
228 - 231 |
Multilayer electron-beam curing of polymer dielectric for electrical interconnections Manepalli R, Farnsworth KD, Allen SAB, Kohl PA |
232 - 234 |
Effect of pH and ionic strength on chemical mechanical polishing of tantalum Ramarajan S, Li Y, Hariharaputhiran M, Her YS, Babu SV |
235 - 238 |
Improvements of amorphous-silicon inverted-staggered thin-film transistors using high-temperature-deposited Al gate with chemical mechanical polishing Shih PS, Chang TC, Liang CY, Huang TY, Chang CY |
239 - 241 |
Preparation of white light electroluminescent europium silicate thin films Qi JF, Matsumoto T, Tanaka M, Masumoto Y |
242 - 244 |
Reduction process of Ruddlesden-Popper-type planar faults in SrTiO3 : Pr3+ by Al addition Okamoto S, Tanaka S, Yamamoto H |
245 - 247 |
Simultaneous detection of nitric oxide concentration and temperature using a single sensor element of SrSnO3-Fe2O3 oxide mixture Ishihara T, Kamakura K, Nishiguchi H, Takita Y |