화학공학소재연구정보센터
Thin Solid Films, Vol.518, No.23, 6839-6843, 2010
Aerosol assisted fabrication of metallic film/carbon fiber and heat treatment to form crystalline alloy film
Carbon fiber (CF) was catalytically activated with spark generated Pd aerosol nanoparticles Metal (Ag, Au, Cu, and Pd) and alloy (Ni-P, Ni-Cu-P) electroless films were deposited on Pd aerosol activated CF using a range of deposition parameters including deposition rate in an electroless deposition bath. Sintering was applied to the alloy films on the CF to examine the crystallization behavior at 400 degrees C in a nitrogen atmosphere. Ni-Cu-P had a higher crystallinity than Ni-P after the treatment (C) 2010 Elsevier B.V. All rights reserved.