화학공학소재연구정보센터
Korean Journal of Chemical Engineering, Vol.31, No.11, 2051-2056, November, 2014
Adsorption and photodegradation of methylene blue on TiO2-halloysite adsorbents
E-mail:
TiO2-halloysite (TiO2-HNT) composites were fabricated by depositing anatase TiO2 on the halloysite (HNT) surfaces with calcination treatment at 100, 200, 300 and 500 ℃. The obtained composites were characterized by transmission electron microscopy (TEM), Fourier transform infrared spectroscopy (FTIR) and X-Ray diffraction (XRD). HNT was attached with TiO2 particles or clusters in sizes of 10-30 nm. With the increasing of calcination temperature, the crystalline of anatase became more perfect, but the structure of HNT could be destroyed at 500 ℃. The adsorption and photodegradation of methylene blue (MB) by TiO2-HNTs were investigated. The kinetic adsorption fit the pseudo second-order, and the isotherm data followed the Langmuir model. The maximum adsorption capacities of MB were in the range of 38.57 to 54.29 mg/g. TiO2-HNTs exhibited an efficient photocatalytic activity in the decomposition of MB. For TiO2-HNT calcined at 300 ℃, 81.6% MB were degraded after 4 h treatment of UV irradiation.
  1. Belkassa K, Bessaha F, Marouf-Khelifa K, Batonneau-Gener I, Comparot J, Khelifa A, Colloids Surf., A, 421, 26 (2013)
  2. Gong JL, Wang B, Zeng GM, Yang CP, Niu CG, Niu QY, Zhou WJ, Liang Y, J. Hazard. Mater., 164(2-3), 1517 (2009)
  3. Crini G, Bioresour. Technol., 97(9), 1061 (2006)
  4. Zhao MF, Liu P, Micropor. Mesopor. Mater., 112, 419 (2008)
  5. Zhang AB, Pan L, Zhang HY, Liu ST, Ye Y, Xia MS, Chen XG, Colloids Surf., A, 396, 182 (2012)
  6. Wang JH, Zhang XA, Zhang B, Zhao YF, Zhai R, Liu JD, Chen RF, Desalination, 259(1-3), 22 (2010)
  7. Massaro M, Riela S, Cavallaro G, Gruttadauria M, Milioto S, Noto R, Lazzara G, J. Organomet. Chem., 749, 410 (2014)
  8. Shamsi MH, Geckeler KE, Nanotechnology, 19, 075604 (2008)
  9. Luo P, Zhao YF, Zhang B, Liu JD, Yang Y, Liu JF, Water Res., 44, 1489 (2010)
  10. Nakata K, Fujishima A, J. Photochem. Photobiol. C, 13, 169 (2012)
  11. Zhang YL, Guo YD, Zhang GK, Gao YY, Appl. Clay Sci., 51, 335 (2011)
  12. Papoulis D, Komarneni S, Panagiotaras D, Stathatos E, Toli D, Christoforidis KC, Fernandez-Garcia M, Li HH, Yin S, Sato T, Katsuki H, Appl. Catal. B: Environ., 132, 416 (2013)
  13. Wang RJ, Jiang GH, Ding YW, Wang Y, Sun XK, Wang XH, Chen WX, ACS Appl. Mater. Inter., 3, 4154 (2011)
  14. Sookhakian M, Amin YM, Basirun WJ, Appl. Clay Sci., 283, 668 (2013)
  15. Zhang Y, Fu LJ, Myang H, Colloids Surf., A, 414, 115 (2012)
  16. Tierrablanca E, Romero-Garcia J, Roman P, Cruz-Silva R, Appl. Catal. A: Gen., 381(1-2), 267 (2010)
  17. Zhang Y, Barber A, Maxted J, Lowe C, Smith R, Li TZ, Prog. Org. Coat., 76, 131 (2013)
  18. Liu L, Wan YZ, Xie YD, Zhai R, Zhang B, Liu JD, Chem. Eng. J., 187, 210 (2012)
  19. Wu DL, Zheng PW, Chang PR, Ma XF, Chem. Eng. J., 174(1), 489 (2011)
  20. Xie YF, Qian DY, Wu DL, Ma XF, Chem. Eng. J., 168(2), 959 (2011)
  21. Bulut Y, Aydin H, Desalination, 194(1-3), 259 (2006)
  22. Wang JM, Li C, Zhuang H, Zhang JH, Food Control, 34, 372 (2013)