동(Cu) 및 동합금(Bronze)의 부식생성물과 탈염처리
Corrosion Products and Desalting Treatments of Copper and Copper Alloy (Bronze)
E-mail:
Benzotriazole (B.T.A) which has been mainly used for the stabilization processing method of excavated copper and bronze artifacts is vaporized within 2~3 years after the usage because it is unstable at the acid conditions and cannot protect the surface of artifacts. In this study, NaOH method which has been used for the steel artifacts was applied as a stabilization process for the method of copper and bronze artifacts to gush chlorine ion out. For the reproduction of excavated samples, copper and bronze plates were dipped in 0.1M HCl for 26 hrs to form CuCl, rusted at 70oC with RH 75% for the formation of corrosion products, and desalted in 0.1 M NaOH solution. The concentration of chlorine ion was measured by using ionchromatography. During the desalting process, a large quantity of chlorine ions was gushed out in early period and corrosion products were not additionally generated through the re-corrosion experiment. This NaOH desalting process was found to be a method of stabilization process for copper and bronze artifacts from the formation of Tenorite (CuO) during desalting as a protection layer for corrosion.
  1. Warraky AE, Shayeb HAE, Sherif EM, Anticorrosion Method. M., 51, 52 (2004)
  2. Black J, Recent Advances in the Conservation and Analysis of Artifacts, p. 135, University of London, London (1987). (1987)
  3. Scott DA, J. Am. Inst. Conservat., 29, 193 (1990)
  4. Fox PG, Lewist G, Boden PJ, Corros. Sci., 19, 457 (1979)
  5. Faltermeier RB, Stud. Conserv., 43, 121 (1998)
  6. Lee OH, Conservation Science of Cultural Property (in Korean),, p. 153, Juluesung, Seoul, (2008). (2008)
  7. Moon WS, Whang JJ, Kim SD, Kang DI, Jung KJ, Jung YD, Conservation Studies, (in Korean), 16, 51 (1995)
  8. Kang MG, Park HH, Korean J. Mater. Res., (in Korean), 6(2), 158 (1996)
  9. Debiemme-Chouvy C, Ammeloot F, Sutter EMM, Appl. Surf. Sci., 174(1), 55 (2001)
  10. Liu B, Zeng HC, J. Am. Chem. Soc., 126(26), 8124 (2004)
  11. stoffyn-Egli P, Buckley DE, Clyburne JAC, Appl. Geochem., 13, 643 (1998)
  12. Rodriguez JA, Kim JY, Hanson JC, Perez M, Frenkel AI, Catal. Lett., 85(3-4), 247 (2003)
  13. Mabille I, Bertrand A, Sutter EMM, Fiaud C, Corros. Sci., 45, 855 (2003)
  14. Moon WS, Whang JJ, Jung YD, Conservation Studies, (in Korean), 17, 3 (1996)
  15. MacLead ID, Stud. Conserv., 32, 25 (1987)
  16. Constantinides I, Adriaens A, Adams F, Appl. Surf. Sci., 189(1-2), 90 (2002)
  17. Robbiola L, Blengino JM, Fiaud C, Corros. Sci., 40, 2083 (1998)