Solid State Ionics, Vol.269, 106-109, 2015
Ionic conductivities in crystalline, glassy, and liquid AgAsS2
Ionic conductivity in AgAsS2 has been measured at 20-600 degrees C for crystalline, glassy, supercooled, and liquid states. The liquids possess substantially smaller activation energies (similar to 02 eV) and conductivity prefactors (similar to 3 S/cm) than those in the solids. Other electrical characteristics are discussed, taking calorimetric and dilatometric results into account. (C) 2014 Elsevier B.V. All rights reserved.
Keywords:Chalcogenide glass;Chalcogenide liquid;Ionic conductivity;Temperature dependence;Thermal analyses