Advanced Materials, Vol.28, No.28, 5939-5939, 2016
High Pressure Chemical Vapor Deposition of Hydrogenated Amorphous Silicon Films and Solar Cells
Thin films of hydrogenated amorphous silicon can be produced at MPa pressures from silane without the use of plasma at temperatures as low as 345 degrees C. High pressure chemical vapor deposition may open a new way to low cost deposition of amorphous silicon solar cells and other thin film structures over very large areas in very compact, simple reactors. [GRAPHICS] .