Journal of Industrial and Engineering Chemistry, Vol.58, 357-368, February, 2018
Environmentally benign green inhibitor to attenuate acid corrosion of 6061Aluminum-15%(v) SiC(P) composite
E-mail:
Work undertaken introduces environmentally safe inhibitor to attenuate acid corrosion of Al-CM. Studies were done by PDP and EIS techniques. Conditions were optimized to get maximum inhibition efficiency. Kinetic and thermodynamic parameters were calculated and discussed in detail. SEM, EDX, AFM, XRD and FT-IR techniques were adopted for surface morphology studies. Inulin showed maximum inhibition efficiency of 90% at 303 K. It acted as mixed type of inhibitor, underwent physisorption and followed Langmuir adsorption isotherm. The remarkable surface smoothness of Al-CM was achieved due to adsorption on inhibitor. The work is a contribution to corrosion chemistry using eco-friendly inhibitor.
Keywords:6061Aluminum-15%(v) SiC(P) composite;Adsorption studies;Electrochemical measurement;Green corrosion inhibitor;Surface characterization
- Goulart CM, Esteves-Souza A, Martinez-Huitle CA, Rodrigues CJF, Maciel MAM, Echevarria A, Corrosion Sci., 67, 281 (2013)
- Patni N, Agarwal S, Shah P, Chin. J. Eng., 2013, 1 (2013)
- Schweitzer AP, Marcel Dekkar, New York, NY, USA, 2003.
- Pardo A, Merino MC, Merino S, Viejo F, Carboneras M, Arrabal R, Corrosion Sci., 47, 1750 (2005)
- Bentiss F, Traisnal, Lagrenee M, Br. Corros. J., 35, 315 (2000)
- Pardo A, Merino MC, Lopez MD, Viejo F, Carboneras M, Merino S, Mater. Corros., 54(5), 311 (2005)
- Hunkeler F, Bohni H, Corrosion, 40(10), 534 (1984)
- Pinto GM, Nayak J, Shetty AN, Synth. React. Inorg. Org. Nano Met. Chem., 41, 127 (2011)
- Fouda AS, Abdallah M, Mohamed TY, Fouad E, Prot. Met. Phys. Chem. Surf., 47(6), 803 (2011)
- Raja AS, Rajendran S, Sathiyabama J, Angel P, Int. J. Innov. Res. Sci. Eng. Technol., 3(4), 11455 (2014)
- Khan G, Newaz KMS, Basirun WJ, Ali HBM, Faraj ML, Khan GM, Int. J. Electrochem. Sci., 10, 6120 (2015)
- Oguzie EE, Corrosion Sci., 49, 1527 (2007)
- Prabhu D, Rao P, J. Environ. Chem. Eng., 1, 676 (2013)
- Prabhu D, Rao P, Int. J. Corros., 1 (2013)
- Prabhu D, Rao P, J. Mater. Environ. Sci., 4(5), 732 (2013)
- Singh AK, Mohapatra S, Pani B, J. Ind. Eng. Chem., 33, 288 (2016)
- Prabakaran M, Kim SH, Mugila N, Hemapriya V, Parameswari K, Chitra S, Chung IM, J. Ind. Eng. Chem., 52, 235 (2017)
- Zhao T, Mu G, Corrosion Sci., 41, 1937 (1999)
- Ansari AF, Quraishi MA, Port. Electrochim. Acta, 28, 321 (2010)
- Ma H, Chen S, Yin B, Zhao S, Liu X, Corrosion Sci., 45, 867 (2003)
- Rajendran S, Reenkala SM, Anthony N, Ramaraj R, Corrosion Sci., 44, 2243 (2002)
- US Congress, Office of Technology Assortment, Biopolymers: Making Materials Nature’s Way, (1993).
- Arukalam IO, Madufor IC, Ogbobe O, Oguzie E, Open Corros. J., 6(1), 1 (2014)
- Arukalam IO, Madufor IC, Ogbobe O, Oguzie E, Pig. Res. Technol., 43, 151 (2014)
- Eddy NO, Ameh PO, Odiongenyi AQ, Port. Electrochim. Acta, 32(3), 183 (2014)
- Umoren SA, Obot IB, Ebenso EE, Obi-Egbedi N, Port. Electrochim. Acta, 26, 199 (2008)
- Umoren SA, Obot IB, Ebenso EE, Obi-Egbedi NO, Desalination, 247(1-3), 561 (2009)
- Umoren SA, Ebenso EE, Pig. Res. Technol, 37, 173 (2009)
- Fares MM, Maayta AK, Al-Mustafa JA, Corrosion Sci., 65, 223 (2012)
- Fares MM, Maayta AK, Al-Mustafa JA, Corrosion Sci., 60, 112 (2012)
- Hassan RM, Zaafarany IA, Materials, 6, 2436 (2013)
- Sugama T, J. Mater. Sci., 3, 3995 (1997)
- Sugama T, DuVall JE, Thin Solid Films, 289, 39 (996)
- Umoren SA, Cellulose, 15, 751 (2008)
- Umoren SA, Ogbobe O, Ebenso EE, Trans. SAEST, 41, 74 (2006)
- Arukalam IO, Ijomah NT, Nwanonenyi SC, Obasi HC, Aharanwa BC, Anyanwu PI, Int. J. Sci. Eng. Res., 5(3), 663 (2014)
- Hassannejad H, Ashkan N, Int. J. Electrochem. Sci., 11, 2106 (2016)
- Charitha BP, Chenan A, Rao P, Ind. Eng. Chem. Res., 56(5), 1137 (2017)
- Abd-El-Nabey BA, Goher YM, Fetouha HA, Karam MS, Port. Electrochim. Acta, 33(4), 231 (2016)
- Ajayi OM, Everitt NM, Voisey KT, Eur. Corros., 1 (2016).
- Jain JL, Jain S, Fundamentals of Biochemistry, Carbohydrates-IV Polysac-charides, 6, S. Chand and company, New Delhi, 2005, pp. 115 chapter-8.
- Roberfroid MB, J. Nutr., 137, 2493S (2007)
- Roberfroid MB, Br. J. Nutr., 93, 13 (2003)
- k-Lisac ES, Gazivoda A, Madza rac M, Electrochim. Acta, 47, 4189 (2007)
- Aluminum and Aluminum Alloys, ASM International, 2015.
- Hameed RSA, Ismail EA, Abu- Nawwas AH, Hussin I, Shafey AL, Int. J. Electrochem. Sci., 10, 2098 (2015)
- Muthukrishnan P, Jeyaprabha B, Tharmaraj P, Prakash P, Res. Chem. Intermed., 41, 5961 (2015)
- Sahin M, Bilgic S, Yilmaz H, Appl. Surf. Sci., 195, 1 (2003)
- Li WH, He Q, Pei CL, Hou BR, Electrochim. Acta, 52(22), 6386 (2007)
- Khaled KF, Al-Qahtani MM, Mater. Chem. Phys., 113(1), 150 (2009)
- Noor EA, Mater. Chem. Phys., 114(2-3), 533 (2009)
- Lenderink HJW, Linden MVD, De Wit JHW, J. Electrochim. Acta, 38, 1989 (1993)
- Bessone J, Mayer C, Jutter K, Lorenz W, J. Electrochim. Acta, 28, 171 (1983)
- Mansfeld F, Lin S, Kim K, Shih H, Mater. Corros., 39, 487 (1988)
- Goncalves RS, Azambuja DS, Lucho AMS, Corrosion Sci., 44, 457 (2002)
- Valand T, Heusler KE, J. Electroanal. Chem., 149, 71 (1983)
- Amin MA, Mohsen Q, Hazzazi OA, Mater. Chem. Phys., 114(2-3), 908 (2009)
- Singh AK, Quraishi MA, Corrosion Sci., 52, 152 (2010)
- Asfaram A, Ghaedi M, Ghezelbash GT, Pepe F, Ecotox. Environ. Safe., 139, 219 (2017)
- Dil EA, Ghaedi M, Ghezelbash GR, Asfaram A, Purkait MK, J. Ind. Eng. Chem., 48, 162 (2017)
- Asfaram A, Ghaedi M, Ghezelbash GR, RSC Adv., 6, 23599 (2016)
- Rivera-Grau LM, Casales M, Regla I, Ortega-Toledo DM, Gutierrez JAA, Porcayo-Calderon J, Martinez-Gomez L, Int. J. Electrochem. Sci., 8, 2491 (2013)
- Bessone JB, Salinas DR, Mayer CE, Ebert M, Lorenz W, J. Electrochim. Acta, 37, 2283 (1992)
- Umoren SA, Obot IB, Ebenso EE, Okafor PC, Anti Corros. Methods Mater., 53, 277 (2006)
- Bouklah M, Hammouti B, Lagrenee M, Bentiss F, Corrosion Sci., 48, 2831 (2006)
- Shivakumar SS, Mohana KN, J. Mater. Environ. Sci., 4(3), 448 (2013)
- Ameer MA, Khamis E, Al-Senani G, J. Appl. Electrochem., 32, 149 (2001)
- Dil EA, Ghaedi M, Ghezelbash GR, Asfaram A, Ecotox. Environ. Safe., 139, 158 (2017)
- Asfaram A, Ghaedi M, Azqhandi MHA, Goudarzi A, Hajati S, J. Ind. Eng. Chem., 54, 377 (2017)
- Li X, Deng S, Corrosion Sci., 65, 299 (2012)
- Bentiss F, Traisnel M, Lagrenee M, J. Appl. Electrochem., 31(1), 41 (2001)
- Sherbini EEFE, Mater. Chem. Phys., 60, 286 (1990)
- Abiola OK, Aliyu AOC, Phillips AA, Ogunsipe AO, J. Mater. Environ. Sci., 4(3), 370 (2013)
- Bereket G, Pinarbsi A, Corros. Eng. Sci. Technol/, 39, 308 (2004)
- Bataineh TT, Al-Qudah MA, Nawafleh EM, Al-Rawashdeh NAF, Int. J. Electrochem. Sci., 9, 3543 (2014)
- Lucas KA, Clarke H, John Wiley and Sons Inc., New York, 1993, pp. 4.
- Tschapek M, Wasowski C, Sanchez RMT, J. Electroanal. Chem., 74, 167 (1976)