Korean Journal of Chemical Engineering, Vol.35, No.11, 2303-2312, November, 2018
Pretreatment of low-grade poly(ethylene terephthalate) waste for effective depolymerization to monomers
E-mail:
Pretreatment process of silica-coated PET fabrics, a major low-grade PET waste, was developed using the reaction with NaOH solution. By destroying the structure of silica coating layer, impurities such as silica and pigment dyes could be removed. The removal of impurity was confirmed by X-ray photoelectron spectroscopy (XPS), scanning electron microscopy (SEM), and energy dispersive X-ray spectroscopy (EDX). The pretreated PET fabric samples were used for depolymerization into its monomer, bis(2-hydroxylethyl) terephthalate (BHET), by glycolysis with ethylene glycol (EG), and zinc acetate (ZnAc) catalyst. The quality of BHET was confirmed by DSC, TGA, HPLC and NMR analyses. The highest BHET yield of 89.23% was obtained from pretreated PET fabrics, while glycolysis with raw PET fabric yielded 85.43%. The BHET yield from untreated silica-coated PET fabrics was 60.39%. The pretreatment process enhances the monomer yield by the removal of impurity and also improves the quality of the monomer
- Wang Q, Yao X, Geng Y, Zhou Q, Lu X, Zhang S, Green Chem., 17, 2473 (2015)
- Park SH, Kim SH, Fash. Text., 1, 22 (2014)
- Shamsi R, Sadeghi GMM, RSC Adv., 6, 38399 (2016)
- Imran M, Kim DH, Al-Masry WA, Mahmood A, Hassan A, Haider S, Ramay SM, Polym. Degrad. Stabil., 98, 904 (2013)
- Tharmapuram SR, Jabarin SA, Adv. Polym. Technol., 2, 147 (2003)
- Tharmapuram SR, Jabarin SA, Adv. Polym. Technol., 2, 155 (2003)
- Nikles DE, Farahat MS, Macromol. Mater. Eng., 290, 13 (2005)
- Lee SC, Sze YW, Lin CC, J. Appl. Polym. Sci., 55(8), 1271 (1995)
- Li M, Huang Y, Yu T, Chen S, Ju A, Ge M, RSC Adv., 4, 46476 (2014)
- George PK, Alexandros KN, Irini DS, Dimitris NB, Dimitris SA, Macromol. Mater. Eng., 291, 1338 (2006)
- Bartolome L, Imran M, Lee KG, Sangalang A, Ahn JK, Kim DH, Green Chem., 16, 279 (2014)
- Al-Sabagh AM, Yehia FZ, Harding DRK, Eshaq G, ElMetwally AE, Green Chem., 18, 3997 (2016)
- Park G, Bartolome L, Lee KG, Lee SJ, Kim DH, Park TJ, Nanoscale, 4, 3879 (2012)
- Demertzis PG, Johansson F, Lievens C, Franz R, Packag. Technol. Sci., 10, 45 (1997)
- Gupta S, Indian J. Fibre Text. Res., 26, 156 (2001)
- Fan Q, Kim YK, Perruzzi MK, Lewis AF, J. Imaging Sci. Technol., 47, 400 (2003)
- Wu X, Wang Y, Yang W, Xie B, Yang M, Dan W, Soft Matter, 8, 10457 (2012)
- Gun'ko VM, Mironyuk IF, Zarko VI, Turov VV, Voronin EF, Pakhlov EM, Goncharuk EV, Leboda R, Skubiszewska-Zieba J, Janusz W, Chibowski S, Levchuk YN, Klyueva AV, J. Colloid Interface Sci., 242(1), 90 (2001)
- Nordstrom J, Matic A, Sun J, Forsyth M, MacFarlane DR, Soft Matter, 6, 2293 (2010)
- Kim S, Sung JH, Ahn KH, Lee SJ, Langmuir, 25(11), 6155 (2009)
- Lamminmaki T, Kentta E, Rautkoski H, Bacher J, Teir S, Kettle J, Sarlin J, J. Surf. Eng. Mater. Adv. Technol., 3, 224 (2013)
- Wu YJ, Lovell V, Pekarovicova A, Fleming PD, Joyce M, J. Graphic Technol., 6, 6 (2013)
- Fertani-Gmati M, Brahim K, Khattech I, Jemal M, Thermochim. Acta, 594, 58 (2014)
- Greenberg SA, J. Phys. Chem., 61, 960 (1957)
- Brinker CJ, J. Non-Cryst. Solids, 100, 31 (1988)
- Al-Sabagh AM, Yehia FZ, Eshaq G, Rabie AM, ElMetwall AE, Egypt J. Petroleum, 25, 53 (2016)
- Karayannidis GP, Achilias DS, Macromol. Mater. Eng., 292, 128 (2007)
- Lopez-Fonseca R, Duque-Ingunza I, Rivas B, Arnaiz S, Gutierrez-Ortiz JI, Polym. Degrad. Stabil., 95, 1022 (2010)
- Bartolome L, Imran M, Cho BG, Al-Masry WA, Kim DH, Ed., Material Recycling - Trends and Perspectives, ISBN: 978-953-51-0327-1, InTech (2012).
- Xi G, Lu M, Sun C, Polym. Degrad. Stabil., 87, 117 (2004)
- Fakirov S, ed. Handbook of thermoplastics, CRC Press, 449 (1994).
- Ryu YB, Lee MS, Korean J. Met. Mater., 56, 72 (2018)
- Chen QW, Li XG, Zhang YH, Qian YT, Adv. Mater., 25, 134 (2002)
- Mahmoud MM, Folz DC, Suchicital CTA, Clark DE, J. Am. Ceram. Soc., 95, 95 (2012)
- Jendoubi F, Mgaidi A, Elmaaoui M, Can. J. Chem. Eng., 75(4), 721 (1997)
- Al-Sabagh AM, Yehia FZ, Eissa AMF, Moustafa ME, Eshaq G, Rabie AM, Polym. Degrad. Stabil., 110, 364 (2014)
- Wang H, Liu Y, Li Z, Zhang X, Zhang S, Zhang Y, Eur. Polym. J., 45, 1535 (2009)
- Yue QF, Wang CX, Zhang LN, Ni Y, Jin YX, Polym. Degrad. Stabil., 96, 399 (2011)
- Nabid MR, Bide Y, Fereidouni N, Etemadi B, Polym. Degrad. Stabil., 144, 434 (2017)