Polymer, Vol.177, 208-213, 2019
Preparation of cyclodextrin-based porous polymeric membrane by bulk polymerization of ethyl acrylate in the presence of cyclodextrin
We disclose an efficient synthesis to prepare polymeric membranes containing cyclodextrins (CDs). Bulk polymerization of ethyl acrylate containing peracetylated gamma-CD (PAc gamma CD) yields a porous polymeric membrane containing CDs [CD membrane (BP)]. Krypton adsorption measurements reveal that the CD membrane (BP) has a porous structure. The specific surface area of the CD membrane (BP) is 10 times higher than that of a CD-based polymeric membrane prepared via solution casting using a solution containing poly(ethyl acrylate) and PAc gamma CD. Due to the large specific surface area of the CD membrane (BP) and the molecular recognition of CD, the capabilities and selectivity of CD membrane (BP) to separate bisphenol A as an environmental pollutant from water are demonstrated.