Polymer Bulletin, Vol.35, No.1-2, 73-78, 1995
Synthesis and Characterization of Poly(Ethyl Vinyl Ether) Containing the Nlo-Phore 4’-Oxy-4-Nitrostilbene in the Side-Chain
4’-(2-Vinyloxyethoxy)-4-nitrostilbene 2 was prepared by the reaction of 4’-hydroxy-4-nitrostilbene 1 with 2-iodoethyl vinyl ether. Monomer 2 was polymerized with cationic initiators to obtain a poly(ethyl vinyl ether) with the NLO-phore 4’-oxy-4-nitrostilbene in the side chain. The resulting polymer 3 was soluble in common solvents such as chloroform and DMSO. The inherent viscosities of polymer 3 were in the range of 0.25-0.30 dL/g in chloroform. Polymer 3 showed a good thermal stability in TGA thermogram. Solution-cast films were cloudy and brittle with a T-g of 63 degrees C.