Bioresource Technology, Vol.73, No.2, 187-189, 2000
The oxypropylation of cork residues: preliminary results
Cork particles were oxypropylated under pressure at a relatively high temperature and yielded a mixture of liquid polyols composed of propylene oxide homopolymer (PPO) and cork macromolecules bearing oligo(propylene oxide) grafts.