화학공학소재연구정보센터
Journal of Materials Science, Vol.36, No.20, 5017-5025, 2001
Zn-K EXAFS investigations on ZnS/ZnO containing vitrified ashes from municipal incinerator facilities
Zn-K transmission EXAFS measurements were performed on vitrified ashes from municipal waste incinerator facilities, which contain low amounts of Zn (up to 3 wt%) and sulphur (up to 0.5 wt%) in a ZnS phase. From the Fourier transform it can be concluded that the zinc ions are fourfold co-ordinated by oxygen or sulphur ions. The amount of zinc ions of sulphur environment, e.g. the concentration of ZnS, was determined by Fourier filtering and subsequent parameter fitting. A quantitative analysis of low ZnS concentrations up to 1 wt% has been performed for samples with a molar ratio Zn/S < 5.