초록
활성탄 담지 팔라듐 촉매상에서 하이드라진에 의한 용존산소의 환원반응을, 15- 35℃, 하이드라진/용존산소의 초기 농도비가 1.5-5, 촉매/물의 비율이 0.025-0.2g L-1인 조건에서 조사하였다. 반응차수는 하이드라진에 대해 1/2차, 산소에 대해 1차로 근사할 수 있었으며, 활성화에너지는 52kJ mol-1로 얻어졌다.
The reduction reaction of dissolved oxygen in water by hydrazine over acti- vated carbon-supported palladium catalyst was studied at 15-35℃. The initial concentration ratio of hydrazine to dissolved oxygen was varied within 1.5-5, and the ratio of catalyst mass to water volume within 0.025-0.2g L-1. The reaction order for hydrazine could be approximated to 1/2 and for dissolved oxygen to 1, respectively. Activation energy was determined to be 52kJ mol-1.
  1. Rozenfeld IL, "Corrosion Inhibitors," McGraw-Hill, 239 (1981)
  2. Rollie ME, Patonay G, Warnwe IM, Ind. Eng. Chem. Res., 26, 1 (1987) 
  3. Harhay A, Wolfe C, Power Eng., Dec., 24 (1987)
  4. Desilva SG, Hearp CW, U.S. Patent, 4,574,071 (1986)
  5. Bosster JF, Hamann HC, Kinstler WI, U.S. Patent, 5,108,624 (1992)
  6. King F, Thomson AL, European Patent, 089,830 (1983)
  7. Suh DJ, Park TJ, Ihm SK, J. Catal., 149(2), 486 (1994) 
  8. Dopheide R, Schroter I, Zacharias H, Surf. Sci., 257, 86 (1991) 
  9. Conna A, Martin MA, Pajares JA, Perez-Pariente J, Avalos M, Yacaman MJ, J. Mol. Catal., 48, 199 (1988) 
  10. Vracar LM, Sepa DB, Damjanovic A, J. Electrochem. Soc., 133, 1835 (1986) 
  11. Dalgaard SB, Sanford MO, Mater. Performance, Apr., 32 (1982)