Journal of Membrane Science, Vol.210, No.2, 245-258, 2002
Determination of cake thickness and porosity during cross-flow ultrafiltration on a plane ceramic membrane surface using an electrochemical method
The thickness and the porosity of a deposit during ultrafiltration experiments are determined using an electrochemical method. Twenty microelectrodes are mounted flush to a ceramic plane membrane and maps of deposit thickness are determined for three inlet/outlet distributors configurations. Combining an electrochemical method and a step transient method, the determination of the thickness and the porosity of a particles deposit is performed. These local thickness and porosity values are analyzed thanks to wall shear stress local measurements obtained in a previous work [Sep. Sci. Technol. 37 (10) (2002) 225 1]. The results emphasize the heterogeneity of the deposit thickness, especially in zones of low wall shear stress. Furthermore, the porosity values of the deposit are ranged between 0.3 and 0.8 as a function of the location at the membrane surface.
Keywords:ultrafiltration;plane ceramic membrane;electrochemical method;deposit thickness;deposit porosity