Biotechnology Letters, Vol.25, No.18, 1521-1524, 2003
Polymerization of cardanol using soybean peroxidase and its potential application as anti-biofilm coating material
Soybean peroxidase (20 mg) catalyzed the oxidative polymerization of cardanol in 2-propanol/phospate buffer solution (25 ml, 1: 1 v/v) and yielded 62% polycardanol over 6 h. Cobalt naphthenate (0.5% w/w) catalyzed the crosslinking of polycardanol and the final hardness of crosslinked polycardanol film exceeded 9 H scale as pencil scratch hardness, which shows a high potential as a commercial coating material. In addition, it showed an excellent anti-biofouling activity to Pseudomonas fluorescens compared to other polymeric materials such as polypropylene.