화학공학소재연구정보센터
Journal of Applied Polymer Science, Vol.91, No.1, 242-246, 2004
Electrospinning of ethyl-cyanoethyl cellulose/tetrahydrofuran solutions
In this study, electrospinning was used to fabricate ethyl-cyanoethyl cellulose [(E-CE)C] fiber from a solution of (E-CE)C/tetrahydrofuran. The diameter of the thinnest fiber fabricated during the electrospinning was about 200 nm. It was found that the diameters of the fibers and their distribution depend on the processing parameters and properties of the solution, such as viscosity, temperature, and concentration, for example. The morphology of the fiber was also observed by SEM. (C) 2003 Wiley Periodicals, Inc.