Journal of Materials Science, Vol.45, No.19, 5393-5397, 2010
Oxidation and abrasive wear of Fe-Si and Fe-Al intermetallic alloys
In the present work, intermetallic alloys Fe-Si and Fe-Al (Fe3Si-C-Cr and Fe3Al-C), produced by induction melting, were evaluated regarding their oxidation and abrasive resistance. The tests performed were quasi-isothermal oxidation, cyclic oxidation, and dry sand/rubber wheel abrasion. As reference, the ASTM A297-HH grade stainless steel was tested in the same conditions. In the oxidation tests, the Fe-Al based alloy presented the lowest oxidation rate, and the Fe-Si based alloy achieved the best results in the abrasion test, showing better performance than the HH type stainless steel.