화학공학소재연구정보센터
학회 한국화학공학회
학술대회 2006년 가을 (10/27 ~ 10/28, 고려대학교)
권호 12권 2호, p.2093
발표분야 에너지/환경
제목 Catalytic degradation of an LDPE-LLDPE-EVA copolymer mixture with used-HZSM-5 andGa/HZSM-5 catalysts
초록 The present work is aimed at studying the performance of used-HZSM-5 catalyst and Ga/HZSM-5 in the catalytic cracking of an LDPE-LLDPE-EVA copolymer mixture, with a composition similar to that found in real agricultural film wastes. The crystallinity, amount of acid site and surface area of a used-HZSM-5 decreaesd a little than those of a fresh HZSM-5, but the catalytic performance of a used-HZSM-5 could be achieved in pyrolysis of polymer mixture. The selectivity to isobutene over used-HZSM-5 was much higher than that of thermal degradation. When pyrolysis vapor was upgraded with HZSM-5 or Ga/HZSM-5, the amount of aromatics in product increased. Product yields over Ga/HZSM-5 shows higher amount of aromatic components such as benzene, toluene, xylene(BTX) than HZSM-5.
저자 전종기1, 김현진1, 김민지1, 박영권2
소속 1공주대, 2서울시립대
키워드 HZSM-5; Ga; pyrolysis
E-Mail
원문파일 초록 보기