Release of BSA-FITC incorporated in calcium phosphate microsphere |
초록 |
This work presents release of BSA-FITC incorporated in CaP microsphere depending on storage time by measuring absorbance of supernatants at 280nm or performing micro BCA protein assay.Calcium phosphate microspheres were prepared by emulsification (water-in-oil) and subsequent nucleation. The emulsification and nucleation were simulated by pH change due to enzyme reaction which makes pH vary from 4 to 7. In order to find optimum condition to form the microsphere, we varied ratio of enzyme to substrate. Obtained BSA-FITC incorporated calcium phosphate microspheres are shown the homogeneous particles sizes in the range of 200-300㎛ in SEM images. We conformed decomposition of urea by urease using FT-IR and incorporation of BSA-FITC into the microsphere using confocal fluorescent microscope. The BSA-FITC incorporated CaP microspheres were stored at 37 ℃ for one month. During the storage, we took 2 mL of supernatant each sampling time for analyzing release of BSA-FITC from the microsphere. We believe that these materials could be potentially applied to the biomedical fields as an injectable bone filler with the controlled drug release materials. |
저자 |
고일환1, 이진형2, 장정호3
|
소속 |
1Bio-IT Convergence Center, 2Korea Institute of Ceramic Engineering and Technology / Department of Chemical Engineering, 3Inha Univ. |
키워드 |
Drug delivery; bone pillar; CaP
|
E-Mail |
|
원문파일 |
초록 보기 |