1 |
First-principles calculations on Ni/W interfaces in Steel/Ni/W hot isostatic pressure diffusion bonding layer Yang J, Wang Y, Huang JH, Ye Z, Sun X, Chen SH, Zhao Y Applied Surface Science, 475, 906, 2019 |
2 |
Direct three-dimensional imaging of the fracture of fiber-reinforced plastic under uniaxial extension: Effect of adhesion between fibers and matrix Saito H, Aoyanagi Y, Mihara T, Tanaka T, Higuchi T, Morita H, Jinnai H Polymer, 116, 556, 2017 |
3 |
Preparation and fracture process of high strength hyaluronic acid hydrogels cross-linked by ethylene glycol diglycidyl ether Tavsanli B, Okay O Reactive & Functional Polymers, 109, 42, 2016 |
4 |
Multifractal analysis of the tensile fracture morphology of polyvinylidene chloride/glass fiber composite Zhang YH, Bai BF, Li JQ, Chen JB, Shen CY Applied Surface Science, 257(7), 2984, 2011 |
5 |
Multifractal analysis of fracture morphology of poly(ethylene-co-vinyl acetate)/carbon black conductive composite Zhang YH, Bai BF, Chen JB, Shen CY, Li JQ Applied Surface Science, 256(23), 7151, 2010 |
6 |
Fracture process of nonstoichiometric oxide based solid oxide fuel cell under oxidizing/reducing gradient conditions Sato K, Yashiro K, Kawada T, Yugami H, Hashida T, Mizusaki J Journal of Power Sources, 195(17), 5481, 2010 |
7 |
Substrate constraint and adhesive thickness effects on fracture toughness of adhesive joints Duan K, Hu XZ, Mai YW Journal of Adhesion Science and Technology, 18(1), 39, 2004 |
8 |
SiC 휘스커 강화 Al 2 O 3 복합재료의 고인화 김연직, 송준희 Korean Journal of Materials Research, 14(9), 649, 2004 |
9 |
Scanning electron micrographs of high density polyethylene fracture surfaces Brough I, Haward RN, Healey G, Wood A Polymer, 45(10), 3115, 2004 |
10 |
Characterization of microscopic failure process and deformation in glass/nylon composites by micro-grid method Takeda N, Ogihara S, Nakata K, Kobayasi A Composite Interfaces, 5(4), 305, 1998 |