2113 - 2123 |
Liquid-liquid phase separation in polysulfone/polyethersulfone/N-methyl-2-pyrrolidone/water quaternary system Baik KJ, Kim JY, Lee HK, Kim SC |
2124 - 2132 |
Formation of polyurethane membranes by immersion precipitation. II. Morphology formation Kim YD, Kim JY, Lee HK, Kim SC |
2133 - 2142 |
Laser interferometric technique for measuring polymer cure kinetics Dudi O, Grubbs WT |
2143 - 2149 |
Polyisoprene, poly(styrene-cobutadiene) and their blends. III. Tensile properties of tetramethylthiuram disulfide/sulfur and 2-bisbenzothiazole-2,2 '-disulfide/sulfur compounds Mallon PE, McGill WJ |
2150 - 2157 |
The effect of grafted TMPM on the radiation resistance of polypropylene Wang HL, Chen WX |
2158 - 2169 |
Permeation barrier properties of polyethylene/modified blends of polyamide and polyvinylalcohol containers against methanol/gasoline fuels Yeh JT, Jou WS, Su YS |
2170 - 2180 |
Thermoreversible hydrogels. VIII. Effect of a zwitterionic monomer on swelling behaviors of thermosensitive hydrogels copolymerized by N-isopropylacrylamide with N,N '-dimethyl (acrylamidopropyl) ammonium propane sulfonate Lee WF, Yeh PL |
2181 - 2195 |
Formation of macroporous styrene-divinylbenzene copolymer networks: Theory vs. experiments Okay O |
2196 - 2206 |
Preparation and epoxy curing of p-nonylphenol/dicyclopentadiene adducts Tseng FP, Chang FC, Lin SF, Lin JJ |
2207 - 2219 |
The influence of maltodextrins on the structure and properties of compression-molded starch plastic sheets van Soest JJG, Kortleve PM |
2220 - 2233 |
Effect of polyvinylpyrrolidone molecular weights on morphology, oil/water separation, mechanical and thermal properties of polyetherimide/polyvinylpyrrolidone hollow fiber membranes Xu ZL, Chung TS, Huang Y |
2234 - 2242 |
The morphology of irradiated isotactic polypropylene Zhang XC, Cameron RE |
2243 - 2254 |
Atomic force microscopy (AFM) studies of liquid crystalline polymer (LCP) surfaces Gould SAC, Shulman JB, Schiraldi DA, Occelli ML |
2255 - 2257 |
A computational study of 2,5-dibenzylidenecyclopentanone and 2,6-dibenzylidenecyclohexanone, model compounds for poly(arylidenecycloalkanones) Sanford EM, Paulisse KW, Reeves JT |
2258 - 2265 |
Modification of polyacrylonitrile (PAN) fiber by blending with N-(2-hydroxy)propyl-3-trimethylammonium chitosan chloride Nam CW, Kim YH, Ko SW |
2266 - 2273 |
New thermosetting resin from terpenediphenol-based benzoxazine and epoxy resin Kimura H, Murata Y, Matsumoto A, Hasegawa K, Ohtsuka K, Fukuda A |
2274 - 2282 |
Mechanical performance of ternary in situ polycarbonate/ poly(acrylonitrile-butadiene-styrene)/liquid crystalline polymer composites Tjong SC, Jiang W |
2283 - 2289 |
Hydrogen bonding in polyamide toughened novolac type phenolic resin Wang FY, Ma CCM, Wu HD |
2290 - 2300 |
Amphipathic polymers with stimuli-responsive microdomains for water remediation: Binding studies with p-cresol Richardson MF, Armentrout RS, McCormick CL |
2301 - 2311 |
Esterification of wheat straw hemicelluloses in the N,N-dimethylformamide/lithium chloride homogeneous system Fang JM, Sun RC, Fowler P, Tomkinson J, Hill CAS |
2312 - 2320 |
Comparative studies on the degradability of poly(ester amide)s derived from L- and L,D-alanine Rodriguez-Galan A, Pelfort M, Aceituno JE, Puiggali J |
2321 - 2332 |
Effect of elastomer modification on the adhesive characteristics of maleimide-functional phenolic resins Gouri C, Nair CPR, Ramaswamy R |