1021 - 1028 |
Self-propagating high-temperature synthesis of aluminum nitride under lower nitrogen pressures Shin J, Ahn DH, Shin MS, Kim YS |
1029 - 1032 |
Low-temperature synthesis of bismuth titanate niobate (Bi7Ti4NbO21) nanoparticles from a metal-organic polymeric precursor Duran P, Moure C, Villegas M, Tartaj J, Caballero AC, Fernandez JF |
1033 - 1038 |
Effect of slurry rheological properties on the coating of ceramic honeycombs with yttria-stabilized-zirconia washcoats Agrafiotis C, Tsetsekou A, Leon I |
1039 - 1043 |
Role of carbon in the sintering of boron-doped silicon carbide Clegg WJ |
1044 - 1048 |
Infiltration and pyrolysis of polytitanocarbosilane in an Si-Ti-C-O fabric/mullite porous composite Hirata Y, Matsura T, Hayata K |
1049 - 1055 |
Fine strontium ferrite powders from an ethanol-based microemulsion Fang JY, Wang J, Gan LM, Ng SC, Ding J, Liu XY |
1056 - 1062 |
Single-step dip coating of crack-free BaTiO3 films > 1 mu m thick: Effect of poly(vinylpyrrolidone) on critical thickness Kozuka H, Kajimura M |
1063 - 1069 |
Effect of hydrogen atmosphere on pyrolysis of cured polycarbosilane fibers Takeda M, Saeki A, Sakamoto J, Imai Y, Ichikawa H |
1070 - 1076 |
Aging of lime putty: Effects on traditional lime mortar carbonation Cazalla O, Rodriguez-Navarro C, Sebastian E, Cultrone G, De la Torre MJ |
1077 - 1080 |
ZrO2 nanopowders prepared by low-temperature vapor-phase hydrolysis Xia B, Duan LY, Xie YC |
1081 - 1086 |
Extrusion of metal-ceramic composite pipes Chen ZC, Ikeda K, Murakami T, Takeda T |
1087 - 1092 |
Synthesis and structural characterization of trimetallic perovskite-type rare-earth orthoferrites, LaxSm1-xFeO3 Traversa E, Nunziante P, Sangaletti L, Allieri B, Depero LE, Aono H, Sadaoka Y |
1093 - 1097 |
Formation of novel ZSM-5/porous mullite composite from sintered kaolin honeycomb by hydrothermal reaction Katsuki H, Furuta S, Komarneni S |
1098 - 1102 |
Synthesis of titanate derivatives using ion-exchange reaction Lee CT, Um MH, Kumazawa H |
1103 - 1107 |
Reactive synthesis and phase stability investigations in the aluminum nitride-silicon carbide system Carrillo-Heian EM, Xue HY, Ohyanagi M, Munir ZA |
1108 - 1112 |
Synthesis of aluminum nitride-silicon carbide solid solutions by combustion nitridation Ohyanagi M, Shirai K, Balandina N, Hisa M, Munir ZA |
1113 - 1116 |
Enhanced magnetization of 3 mol% yttria-doped zirconia/barium hexaferrite by post-plastic deformation Suzuki Y, Awano M, Kondo N, Ohji T |
1117 - 1121 |
Aluminum nitride whisker formation during combustion synthesis Lee KJ, Ahn DH, Kim YS |
1122 - 1128 |
Characterization of fine-grained bismuth vanadate ceramics obtained using nanosized powders Shantha K, Varma KBR |
1129 - 1136 |
Equilibrium point defect and electronic carrier distributions near interfaces in acceptor-doped strontium titanate McIntyre PC |
1137 - 1144 |
Effect of the interfacial transition zone on the conductivity of portland cement mortars Shane JD, Mason TO, Jennings HM, Garboczi EJ, Bentz DP |
1145 - 1148 |
Effects of B2O3 addition on the dielectric and ferroelectric properties of Ba0.7Sr0.3TiO3 ceramics Rhim SM, Hong S, Bak H, Kim OK |
1149 - 1152 |
Dielectric properties of Pb(Fe2/3W1/3)O-3-PbTiO3 solid-solution ceramics Vilarinho PM, Zhou LQ, Pockl M, Marques N, Baptista JL |
1153 - 1159 |
Finite-element analysis of ceramic multilayer capacitors: Modeling and electrical impedance spectroscopy for a nondestructive failure test Prume K, Waser R, Franken K, Maier HR |
1160 - 1164 |
Corrosion of ceramics in aqueous hydrofluoric acid Mikeska KR, Bennison SJ, Grise SL |
1165 - 1170 |
Piezospectroscopic analysis of interface debonding in thermal barrier coatings Peng X, Clarke DR |
1171 - 1176 |
Microstructure and oxidation behavior of silicon carbide fibers derived from polycarbosilane Takeda M, Urano A, Sakamoto J, Imai Y |
1177 - 1185 |
Flexural fracture strength, fracture locations, and Monte Carlo predictions for a silicon nitride by ten US laboratories Tennery VJ, Breder K, Ferber MK, Jenkins MG |
1186 - 1191 |
Tensile fracture behavior of two types of silicon nitride specimen geometries conducted by ten US groups Tennery VJ, Breder K, Ferber MK, Jenkins MG |
1192 - 1198 |
Kinetics of enthalpy relaxation at the class transition in ternary tellurite glasses Aida K, Benino Y, Dimitrov V, Komatsu T, Sato R |
1199 - 1206 |
Fracture resistance and stable crack-growth behavior of 8-mol%-yttria-stabilized zirconia Kumar AN, Sorensen BF |
1207 - 1214 |
Effect of fiber bridging stress on the fracture resistance of silicon-carbide-fiber/zircon composites Wang YL, Anandakumar U, Singh RN |
1215 - 1218 |
Effects of an electric field on the fracture toughness of poled lead zirconate titanate ceramics Fu R, Zhang TY |
1219 - 1225 |
Polishing behavior and surface quality of alumina and alumina/silicon carbide nanocomposites Kara H, Roberts SG |
1226 - 1232 |
Experimental method for determining surface energy anisotropy and its application to magnesia Saylor DM, Mason DE, Rohrer GS |
1233 - 1236 |
Effect of monovalent cation additives on the gamma-Al2O3-to-alpha-Al2O3 phase transition Okada K, Hattori A, Kameshima Y, Yasumori A, Das RN |
1237 - 1240 |
Mullitization from a multicomponent oxide system in the temperature range 1200 degrees-1500 degrees C Shin H, Kim CS, Chang SN |
1241 - 1246 |
Characterization of photoluminescent (Y1-xEux)(2)O-3 thin films prepared by metallorganic chemical vapor deposition McKittrick J, Bacalski CF, Hirata GA, Hubbard KM, Pattillo SG, Salazar KV, Trkula M |
1247 - 1252 |
Coarsening behavior of tricalcium silicate (C3S) and dicalcium silicate (C2S) grains dispersed in a clinker melt Kwon SK, Hong SH, Kim DY, Hwang NM |
1253 - 1258 |
Superstructure in a triclinic phase of tricalcium silicate Urabe K, Shirakami T, Iwashima M |
1259 - 1265 |
Effects of (B2O3, P2O5) additives on microstructural development and phase-transformation kinetics of stoichiometric cordierite glasses Wu JM, Hwang SP |
1266 - 1272 |
Characteristic spherulitic microstructure in partial-melt-processed YBa2Cu3Ox/HfO2 Yan Y, Evetts JE, Zhang JI, Stobbs WM |
1273 - 1275 |
Imaging secondary-ion mass spectroscopy observation of the scavenging of siliceous film from 8-mol%-yttria-stabilized zirconia by the addition of alumina Lee JH, Mori T, Li JG, Ikegami T, Komatsu M, Haneda H |
1276 - 1278 |
Synthesis of yttrium aluminum garnet from a mixed-metal citrate precursor Cinibulk MK |
1279 - 1280 |
Al2O3-Ni composites with high strength and fracture toughness Fahrenholtz WG, Ellerby DT, Loehman RE |
1281 - 1283 |
Field-assisted sintering of nanocrystalline titanium nitride Groza JR, Curtis JD, Kramer M |
1284 - 1286 |
Pr3+/Er3+ codoped Ge-As-Ga-S glasses as dual-wavelength fiber-optic amplifiers for 1.31 and 1.55 mu m windows Park SH, Lee DC, Heo J |
1287 - 1289 |
Preparation and spherical agglomeration of crystalline cerium(IV) oxide nanoparticles by thermal hydrolysis Hirano M, Fukuda Y, Iwata H, Hotta Y, Inagaki M |
1290 - 1292 |
Formation of nanometric TiB2 from TiO2 Welham NJ |
1293 - 1295 |
Forming Al2O3-Al composites with controlled compositions by reactive metal penetration of dense aluminosilicate preforms Fahrenholtz WG, Ellerby DT, Ewsuk KG, Loehman RE |
1296 - 1298 |
Formation of convoluted silica precipitates during amorphous phase separation in the Ca-3(PO4)(2)-Sio(2)-MgO system Oliveira JM, Correia RN, Fernandes MHV |
1299 - 1301 |
Scanning electron-beam dielectric microscopy for the investigation of the temperature coefficient distribution of dielectric ceramics Cho Y, Jintsugawa O, Yamanouchi K |
1302 - 1304 |
Influence of apparent pressure on wear behavior of self-mated alumina Ravikiran A |
1305 - 1307 |
Infrared spectroscopic method for determination of thermal properties of fluorophosphate glasses Karmakar B, Kundu P, Dwivedi RN |
1308 - 1310 |
Microscopic study of SnO2 crystals in the cold decoration layer of bone China Chung YC, Im DH, Kim CK, Yoon CS |
1311 - 1313 |
Toughening and strengthening of NiAl with Al2O3 by the addition of ZrO2(3Y) Kitaoka A, Hirota K, Yoshinaka M, Miyamoto Y, Yamaguchi O |
1314 - 1316 |
Strengthening of porous alumina by pulse electric current sintering and nanocomposite processing Oh ST, Tajima K, Ando M, Ohji T |
1317 - 1319 |
X-ray studies of ferroelectric cathodes Zhang SR, Cai XM, Zhong CW, Zhu WY |
1320 - 1322 |
Colloid emulsion of nanosized strontium bismuth tantalate powder Lu CH, Saha SK |
1323 - 1323 |
Comment on "Influence of yttrium doping on grain misorientation in aluminum oxide" Lartigue-Korinek S, Priester L |
1324 - 1324 |
Reply to "Comment on'influence of yttrium doping on grain misorientation in aluminum oxide"' Chan HM, Harmer MP, Rickman JM |
1325 - 1325 |
Kinetics and microstructural evolution of heterogeneous transformation of theta-alumina to alpha-alumina (vol 83, pg 362, 2000) Kao HC, Wei WCJ |
1326 - 1326 |
Surface roughening and unstable neck formation in faceted particles: II, mathematical modeling (vol 82, pg 1873, 1999) Sheldon BW, Rankin J |