1453 - 1455 |
Factors affecting the preparation of Sr2Fe2-xMoxO6 Fang TT, Ko TF |
1456 - 1463 |
Phase formation and microstructure of titanium oxides and composites produced by thermal plasma oxidation of titanium carbide Ishigaki T, Li YL, Kataoka E |
1464 - 1467 |
Synthesis of bismuth sodium titanate nanosized powders by solution/sol-gel process Kim CY, Sekino T, Niihara K |
1468 - 1473 |
Pressureless sintering of boron carbide Lee H, Speyer RF |
1474 - 1480 |
Formation of lead zirconate titanate powders by spray pyrolysis Nimmo W, Ali NJ, Brydson RM, Calvert C, Hampartsoumian E, Hind D, Milne SJ |
1481 - 1486 |
Preparation and characterization of macroporous alpha-alumina Sokolov S, Bell D, Stein A |
1487 - 1492 |
Additive-enhanced redispersion of ceramic agglomerates Uhland SA, Cima MJ, Sachs EM |
1493 - 1499 |
Wet-chemical routes leading to scandia nanopowders Li JG, Ikegami T, Mori T, Yajima Y |
1500 - 1503 |
Vaporization processes and pressure buildup during dewatering of dense refractory castables Innocentini MDM, Miranda MFS, Cardoso FA, Pandolfelli VC |
1504 - 1507 |
Proton conductivity in Zr4+-ion-doped P2O5-SiO2 porous glasses Nogami M, Goto Y, Kasuga T |
1508 - 1512 |
Photocatalytic silver recovery using ZnO nanopowders synthesized by modified glycine-nitrate process Park S, Lee DW, Lee JC, Lee JH |
1513 - 1517 |
Field emission characteristics of amorphous diamond Kan MC, Huang JL, Sung J, Lii DF, Chen KH |
1518 - 1521 |
Effect of alumina addition on the distribution of intergranular-liquid phase during sintering of 15-mol%-calcia-stabilized zirconia Lee JH, Lee JH, Jung YS, Kim DY |
1522 - 1526 |
Increase in phase transition temperature of activated alumina with nano-zirconia synthesized by pulsed wire discharge Kinemuchi Y, Mouri H, Suzuki T, Suematsu H, Jiang W, Yatsui K |
1527 - 1533 |
Zeolite synthesized by alkaline hydrothermal treatment of bottom ash from combustion of municipal solid wastes Penilla RP, Bustos AG, Elizalde SG |
1534 - 1539 |
Dispersing behavior of hydroxyapatite powders produced by wet-chemical synthesis Pretto M, Costa AL, Landi E, Tampieri A, Galassi C |
1540 - 1546 |
Crystallization measurements using DTA methods: Applications to Zerodur Davis MJ, Mitra I |
1547 - 1553 |
Influence of residual stresses on the wear behavior of alumina/alumina-zirconia laminated composites Toschi F, Melandri C, Pinasco P, Roncari E, Guicciardi S, de Portu G |
1554 - 1559 |
Effect of Po-2 on bulk and grain boundary resistance of n-type BaTiO3 at cryogenic temperatures Kolodiazhnyi T, Petric A |
1560 - 1566 |
Properties of lead zirconate titanate thin films prepared using a triol sol-gel route Naksata M, Brydson R, Milne SJ |
1567 - 1570 |
CeO2-CoO phase diagram Chen M, Hallstedt B, Grundy AN, Gauckler LJ |
1571 - 1577 |
Texture development in modified lead titanate thin films obtained by chemical solution deposition on silicon-based substrates Ricote J, Poyato R, Aguero M, Pardo L, Calzada ML, Chateigner D |
1578 - 1585 |
Formation of beta-silicon nitride crystals from (Si,Al,Mg,Y)(O,N) liquid: I, phase, composition, and shape evolutions Wang LL, Tien TY, Chen IW |
1586 - 1591 |
Formation of beta-silicon nitride crystals from (Si,Al,Mg,Y)(O,N) liquid: II, population dynamics and coarsening kinetics Wang LL, Tien TY, Chen IW |
1592 - 1594 |
Hydrothermal chemistry of silicates: Low-temperature synthesis of y-yttrium disilicate Becerro AI, Naranjo M, Perdigon AC, Trillo JM |
1595 - 1597 |
Yttrium silicate powders produced by the sol-gel method, structural and thermal characterization Boyer D, Derby B |
1598 - 1600 |
Characterization of precursor-derived silicon-carbon-nitrogen ceramics after creep testing Cai Y, Zimmermann A, Bauer A, Aldinger F |
1601 - 1604 |
Use of the retarded solution-reprecipitation process to attain a higher initial permeability in MnZn ferrites Drofenik M, Znidarsic A, Makovec D |
1605 - 1608 |
Anatase sol prepared from peroxotitanium complex aqueous solution containing niobium or vanadium Ichinose H, Taira M, Furuta S, Katsuki H |
1609 - 1611 |
Spark plasma sintering of nano-sized TiN prepared from TiO2 by controlled hydrolysis of TiCl4 and Ti(O-i-C3H7)(4) solution Kawano S, Takahashi J, Shimada S |
1612 - 1615 |
Application of a tough surface layer to a fiber-bonded composite Kim Y, Kagawa Y, Zhu S |
1616 - 1618 |
Current-voltage characteristics of cobalt-doped inversion boundaries in zinc oxide bicrystals Oba F, Sato Y, Yamamoto T, Ikuhara Y, Sakuma T |
1619 - 1621 |
Strength of silicon nitride after thermal shock She JH, Yang JF, Jayaseelan DD, Ueno S, Kondo N, Ohji T, Kanzaki S |
1622 - 1624 |
Sol-gel alumina coating for improved cyclic oxidation resistance of silicon nitride Tsarenko I, Park S, Du HH, Lee WY |
1625 - 1627 |
Positronium annihilation study of porosity in silica xerogels prepared by a sol-gel process Wakabayashi Y, Ito K, Li HL, Ujihira Y, Kamitani K, Inoue H, Makishima A |
1628 - 1630 |
Combined spectroscopic and thermodynamic investigation of nextel-720 fiber/alumina ceramic-matrix composite in air and water vapor at 1100 degrees C Wannaparhun S, Seal S |
1631 - 1634 |
Fabrication of NiO nanoparticle-coated lead zirconate titanate powders by the heterogeneous precipitation method Xiang PH, Dong XL, Feng CD, Wang YL |
1635 - 1637 |
Microwave plasma synthesis of nanostructured gamma-Al2O3 powders Fu L, Johnson DL, Zheng JG, Dravid VP |
1638 - 1640 |
Nanostructured silicon oxide-nickel oxide sol-gel films with enhanced optical carbon monoxide gas sensitivity Martucci A, Pasquale M, Guglielmi M, Post M, Pivin JC |