화학공학소재연구정보센터
Journal of Industrial and Engineering Chemistry, Vol.20, No.5, 3025-3032, September, 2014
Removal of Cr(VI) from aqueous solution by surfactant-modified kaolinite
E-mail:
Removal of Cr(VI) from aqueous solution by hexadecyltrimethylammonium chloride (HDTMA) modified kaolinite (HMK) was investigated, where the maximum adsorptive capacity reached 27.8 mg/g Cr(VI) using HMK compared with only 0.7 mg/g using unmodified natural kaolinite (NK). The adsorption of Cr(VI) on HMK can be well described by the Langmuir isotherm, and the kinetic adsorption of Cr(VI) on both HMK and NK fitted a pseudo-second-order model. FTIR analysis showed that surface modified HDTMA was responsible for the high adsorptive capacity of Cr(VI). HMK was used to remove Cr(VI) from an electroplating wastewater.
  1. Anirudhan TS, Jalajamony S, Suchithra PS, Colloids Surf. A: Physicochem. Eng. Asp., 335, 107 (2009)
  2. Faghihian H, Bowman RS, Water Res., 39, 1099 (2005)
  3. Mohan D, Pittman CU, J. Hazard. Mater., 137(2), 762 (2006)
  4. Hong H, Jiang W, Zhang X, Tie L, Li Z, Appl. Clay Sci., 42, 292 (2008)
  5. Wang YH, Lan Y, Hu YH, Miner. Eng., 21(12-14), 913 (2008)
  6. Li Z, Jones HK, Zhang P, Bowman RS, Chemosphere, 68, 1861 (2007)
  7. Krishna BS, Murty DSR, Prakash BSJ, Appl. Clay Sci., 20, 65 (2001)
  8. Hamadi NK, Chen X, Farid MM, Lu M, Chem. Eng. J., 81, 95 (2001)
  9. Minamisawa M, Minamisawa H, Yıshida S, Takai N, J. Agric. Food Chem., 52, 5606 (2004)
  10. Malkoc E, Nuhoglu Y, Dundar M, J. Hazard. Mater., 138(1), 142 (2006)
  11. Jiang MQ, Jin XY, Lu XQ, Chen ZL, Desalination, 252(1-3), 33 (2010)
  12. Adebowale KO, Unuabonah IE, Olu-Owolabi BI, J. Hazard. Mater., 134(1-3), 130 (2006)
  13. Jiang MQ, Wang QP, Jin XY, Chen ZL, J. Hazard. Mater., 170(1), 332 (2009)
  14. Lee S, Kim S, Appl. Clay Sci., 22, 55 (2002)
  15. Li Z, Gallus L, Colloids Surf. A: Physicochem. Eng. Asp., 264, 61 (2005)
  16. He H, Ray FL, Zhu J, Spectroc. Acta Pt. A-Molec. Biomolec. Spectr., 60, 2853 (2004)
  17. Yuan P, Annabi-Bergaya F, Tao Q, Fan MD, Liu ZW, Zhu JX, He HP, Chen TH, J. Colloid Interface Sci., 324(1-2), 142 (2008)
  18. Peker S, Yapar S, Besun N, Colloids Surf. A: Physicochem. Eng. Asp., 104, 249 (1995)
  19. Du JH, Morris G, Pushkarova RA, Smart RS, Langmuir, 26(16), 13227 (2010)
  20. Lu H, Luan M, J. China Univ. Mining Technol., 18, 125 (2008)
  21. Wang SB, Li HT, J. Hazard. Mater., 126(1-3), 71 (2005)
  22. Unuabonah EI, Adebowale KO, Olu-Owolabi BI, J. Hazard. Mater., 144(1-2), 386 (2007)
  23. Uysal M, Ar I, J. Hazard. Mater., 149(2), 482 (2007)
  24. Arica MY, Bayramoglu G, Colloids Surf. A: Physicochem. Eng. Asp., 253, 203 (2005)
  25. Granados-Correa F, Jimenez-Becerril J, J. Hazard. Mater., 162(2-3), 1178 (2009)
  26. Weng CH, Sharma YC, Chu SH, J. Hazard. Mater., 155(1-2), 65 (2008)
  27. Unuabonah EI, Adebowale KO, Hydrometallurgy, 93, 1 (2008)
  28. Sari A, Tuzen M, Citak D, Soylak M, J. Hazard. Mater., 149(2), 283 (2007)
  29. Zhao D, Feng S, Chen C, Appl. Clay Sci., 41, 17 (2008)
  30. Bayramoglu G, Arica MY, Chem. Eng. J., 139(1), 20 (2008)
  31. Bhattacharyya KG, Gupta SS, Colloids Surf. A: Physicochem. Eng. Asp., 317, 71 (2008)
  32. Malkoc E, Nuhoglu Y, Dundar M, J. Hazard. Mater., 138(1), 142 (2006)
  33. Atia AA, Appl. Clay Sci., 41, 73 (2008)