3 - 10 |
A method for the analysis of the growth of short fatigue cracks McEvily AJ |
11 - 16 |
Studies of SCC and hydrogen embrittlement of high strength alloys using fracture mechanics methods Dietzel W, Pfuff M, Juilfs GG |
17 - 24 |
A model for crack-induced nucleation of dislocations, complex stacking faults, and twins Beltz GE, Chang M, Machova A |
25 - 32 |
Ideal strength of nano-components Kitamura T, Umeno Y, Kushima A |
33 - 38 |
Theoretical strength of metals and intermetallics from first principles Sob M, Pokluda J, Cerny M, Sandera P, Vitek V |
39 - 44 |
Nanoscale measurement of stress and strain by quantitative high-resolution electron microscopy Hytch M, Putaux JL, Penisson JM |
45 - 50 |
Atomic force microscopy study of the early fatigue damage Polak J, Man J, Obrtlik K |
51 - 54 |
Mechanical response of semi-brittle nano particles under an imposed cyclic field Katz Y, Mook W, Mukherjee R, Gidwani A, Deneen J, Gerberich WW |
55 - 62 |
Prediction and control of grain boundary fracture in brittle materials on the basis of the strongest-link theory Watanabe T, Tsurekawa S |
63 - 70 |
Anisotropic behaviour of grain boundaries Paidar V, Lejcek P |
71 - 76 |
Plasticity of copper with small grain size Champion Y, Langlois C, Guerin S, Lartigue-Korinek S, Langlois P, Hytch MJ |
77 - 82 |
Mechanical behavior of nanostructured aluminum alloys containing quasicrystalline phase Milman YV |
83 - 88 |
Effect of processing route on microstructure and mechanical behaviour of ultrafine grained metals processed by severe plastic deformation Sklenicka V, Dvorak J, Svoboda M, Kral P, Vlach B |
89 - 94 |
Cause and effect of factors affecting the Delta K-th of small crack Kondo Y |
95 - 102 |
The significance of plastic zone growth under cyclic loading and crack opening/closing model in fatigue crack propagation Toyosada M, Gotoh K |
103 - 108 |
Microstructural characterization by nondestructive methods Lukac P, Trojanova Z, Chmelik F |
109 - 114 |
Critical planes in multiaxial fatigue Karolczuk A, Macha E |
115 - 120 |
Fracture behaviour of brittle (glass) matrix composites Dlouhy I, Chlup Z, Boccaccini AR |
123 - 126 |
Breakdown of the Schmid law in bcc molybdenum related to the effect of shear stress perpendicular to the slip direction Groger R, Vitek V |
127 - 130 |
Criterion of mechanical instability in inhomogeneous atomic system Umeno Y, Kitamura T |
131 - 134 |
Ductile-brittle behavior of microcracks in 3D Pelikan V, Hora P, Machova A, Landa M |
135 - 138 |
Elasticity and stability of Fe-P ordered systems from first principles Cerny M, Pokluda J |
139 - 142 |
Ab-initio study of mechanical properties of transition-metal aluminides: a case study for Al-3(V,Ti) Jahnatek M, Krajci M, Hafner J |
143 - 146 |
Locally initiated elastic waves in 2D metals Poletaev GM, Aksenov MS, Starostenkov MD, Patzeva JV |
147 - 150 |
Effect of ordering on the elastic parameters of multicomponent Ni-based systems Bursik J |
151 - 154 |
Near-field study of carrier dynamics in InAs/GaAs quantum dots grown on InGaAs layers Tomanek P, Dobis P, Benesova M, Grmela L |
155 - 158 |
Disorientations and their role on the work-hardening in stage IV Pantleon W |
159 - 162 |
Stability and motion of low angle dislocation boundaries in precipitation hardened crystals Holec D, Dlouhy A |
163 - 166 |
A three dimensional discrete dislocation dynamics analysis of cyclic straining in 316L stainless steel Depres CJ, Robertson CF, Fivel MC, Degallaix S |
167 - 170 |
The migration of solute atoms in the stress field of a slowly moving crack Streitenberger P |
171 - 174 |
Modelling cleavage fracture in high strength steels and their welds Rodriguez-Martin R, Ocana I, Martin-Meizoso A |
175 - 178 |
Micromechanisms of cleavage fracture in HAZ of low carbon steel welds Moya-Gutierrez C, Ocana-Arizcorreta I, Martin-Meizoso A |
179 - 182 |
Dislocation structures of duplex stainless steel in uniaxial and biaxial cyclic loading Petrenec M, Aubin V, Polak J, Degallaix S |
183 - 186 |
Microstructure and thermal stability of ultra fine grained Mg and Mg-Gd alloys prepared by high-pressure torsion Cizek J, Prochazka I, Smola B, Stulikova I, Kuzel R, Matej Z, Cherkaska V, Islamgaliev RK, Kulyasova O |
187 - 190 |
Annealing behaviour of Fe-C-N nanopowder: formation of iron/graphite core-shell structured nanoparticles David B, Pizurova N, Schneeweiss O, Bezdicka P, Filip J, Alexandrescu R, Morjan I, Crunteanu A, Voicu I |
191 - 194 |
Effect of grain boundary segregation on mechanical properties of P-doped Fe-Si base alloys Janovec J, Jenko M, Pokluda J, Vlach B, Lejcek P, Svoboda M, Sandera P |
195 - 198 |
Influence of lattice anisotropy on models formulated by cellular automata in presence of grain boundary movement: a case study Kroc J |
199 - 202 |
Migration of the 45 degrees[100],(001)/(011) asymmetrical tilt grain boundary in an Fe-6at%Si alloy Havlova V, Lejcek P |
203 - 206 |
Study of carbon films on silicon substrates Jasek O, Elias M, Frgala Z, Matejkova J, Rek A, Kadlecikova M |
207 - 210 |
Positron annihilation studies of microstructure of ultra fine grained metals prepared by severe plastic deformation Cizek J, Prochazka I, Smola B, Stulikova I, Kuzel R, Cieslar M, Matej Z, Cherkaska V, Brauer G, Anwand W, Islamgaliev RK, Kulyasova O |
211 - 214 |
Experimental investigation of the local deformation behaviour of MMCs Unterweger K, Kolednik O |
215 - 218 |
Local and global fracture properties in metal matrix composites Sabirov I, Kolednik O |
219 - 222 |
Phase composition and microstructure stability of Al-Ni-Zr alloys Bartova B, Verner J, Vojtech D, Gemperle A, Cernansky M |
223 - 226 |
Interaction of a crack in the plasma-sprayed ceramic coating with the metal substrate Nahlik L, Knesl Z, Kroupa F |
227 - 230 |
3D Visualisation of short crack propagation in Al alloy using high resolution Synchrotron X-ray microtomography Ferrie E, Buffiere JY, Ludwig W |
231 - 234 |
Identification and modelling of the behaviour of a duplex stainless steel by methods of scale changing Jaupitre F, Degallaix S, Kondo D, Quaegebeur P, Forget P |
235 - 238 |
Influence of material state at a crack tip on the process of fatigue striations formation for Al-based alloys Shaniavski AA |
239 - 242 |
Grain size estimation in anisotropic materials Saxl I, Ponizil P, Sulleiova K |
243 - 246 |
Application of silicon for a protection of titanium against high-temperature oxidation Vojtech D, Kubatik T, Cizova H |
247 - 250 |
Biocompatibility of carbon layer on polymer Kubova O, Bacakova L, Svorcik V |
251 - 254 |
Biocompatibility of polyethylene doped with oxycellulose Mikulikova R, Kolarova K, Bacakova L, Svorcik V |
255 - 258 |
Strain heterogeneity and damage localization in nodular cast iron microstructures Nicoletto G, Collini L, Konecna R, Bujnova P |
259 - 262 |
Textural fractography of fatigue failures under variable cycle loading Lauschmann H, Siska F, Nedbal I |
263 - 266 |
Analysis of fracture morphology and local loading modes in torsional fatigue Slamecka K, Pokluda J |
267 - 270 |
Effect of structure on creep behaviour of superalloy single crystals Lukas P, Kunz L, Svoboda M, Cadek J |
271 - 274 |
Microstructural development in tension and compression creep of magnesium alloy AE42 Dieringa H, Bowles A, Hort N, Kainer KU |
275 - 278 |
Microstructure and creep properties of AISI 316LN steels with niobium additions Vodarek V, Roznovska G, Sobotka J |
279 - 282 |
Effect of processing parameters on microstructure and properties of continuously cast Al-Mg sheets Slamova M, Slama P, Homola P, Karlik M |
283 - 286 |
Effects of hydrogen environment on fatigue characteristics of 18Cr-8Ni stainless steel Kawamoto K, Aoki Y, Oda Y, Yoshimura T, Noguchi H, Higashida K |
287 - 290 |
Damage mechanisms and rupture criterion of PM Ti-6Al-4V at 20K Di Lorio S, Briottet L, Rauch EF, Guichard D |
291 - 294 |
Dip-test internal stress and the composite model of creep deformation Dobes F, Orlova A |
295 - 298 |
The formation and destruction of the boundary layer in polymer composite fiber shells during their ageing Senchurov SP, Zabashta YF |
299 - 302 |
On crack path in fibres-reinforced ceramic composites Profant T, Kotoul M |
303 - 306 |
The role of the constraint in the case of short cracks Hutar P, Seitl S, Knesl Z |
307 - 310 |
Critical strain energy density along the curved front of the growing fatigue crack Denk T, Oliva V, Materna A |
311 - 314 |
On the crack tip shielding in particle reinforced composites Hornikova J, Sandera P, Pokluda J |
315 - 318 |
Identification and simulation of elastic-plastic deformation model Maciejewski L, Myszka W, Zietek G |
319 - 322 |
New description of steady-state creep rate, yield stress, stress relaxation, and their interrelation Kohout J |
323 - 326 |
Computational modelling of spherical cavity behaviour in rubber-like solids Pavel S, Jiri B |
327 - 330 |
Tangent moduli of the Hencky material model derived from the stored energy function at finite strains Pozivilova A, Plesek J |
331 - 334 |
Modelling of the Charpy impact test in the DBTT range Hausild P, Berdin C, Rossoll A |
335 - 338 |
Parameters identification for GTN model and their verification on 42CrMo4 steel Kozak V, Vlcek L |
339 - 342 |
A fracture mechanics investigation on crack growth in massive forming Trattnig G, Sommitsch C, Pippan R |
343 - 346 |
Finite element computational technology in resonant ultrasound spectroscopy of composite materials Kolman R, Plesek J, Landa M |
347 - 350 |
Compatibilizer effect of grafted glycidyl methacrylate on EPDM/organoclay nanocomposites Gatos KG, Apostolov AA, Karger-Kocsis J |
351 - 354 |
Elastic properties of structural phases in shape memory alloys investigated by resonant ultrasound spectroscopy Landa M, Novak V, Sedlak P, Manosa L, Sittner P |
355 - 358 |
Effect of interfaces on fiber fracture in Mg and MgLi matrix composites Kudela S, Wendrock H, Kudela S, Ptacek L, Menzel S, Wetzig K |
359 - 362 |
Influence of inclusions on fatigue characteristics of non-combustible Mg alloy Kitahara Y, Shimazaki H, Yabu T, Noguchi H, Sakamoto M, Ueno H |
363 - 366 |
Mechanical properties of AS21 magnesium alloy based composites Trojanova Z, Szaraz Z |
367 - 370 |
Investigation of dynamic strain ageing effects of low alloy steels 15Kh2MFA and 15Kh2NMFA Ernestova M |
371 - 374 |
Influence of isothermal transformation dwell on tensile and fatigue properties of austempered ductile iron Vechet S, Kohout J, Hanzlikova K |
375 - 378 |
Influence of temperature on fracture mechanisms of magnesium composites Gartnerova V, Chalupova M, Jager A, Trojanova Z |
379 - 382 |
Influence of surface skin on the fatigue properties of die-cast magnesium alloy AS21X Lamark TT, Janecek M, Estrin Y |
383 - 386 |
Crack growth anomalies in base steel P91 and in HAZ Balik J, Janecek M, Pesicka J |
387 - 390 |
Damping measurements of the magnesium wrought alloys AZ31, AZ61 and AZ80 after indirect and hydrostatic extrusion Goken J, Swiostek J, Letzig D, Kainer KU |
391 - 394 |
Electrical properties of polymer composites Podgrabinski T, Slepicka P, Rybka V, Svorcik V |
395 - 398 |
Application of giant magnetostrictive material into construction of broad spectrum vibration generator Bomba J, Kaleta J, Sawa P |
399 - 402 |
On a testing of mechanical properties of material surfaces Berka L, Murafa NV |
403 - 406 |
Experimental identification of magnetorheological composites and elastomers properties Kaleta J, Lewandowski D, Zajac P |
407 - 410 |
Relation between uniaxial and equi-biaxial creep and creep fracture behaviour in P91 steel Milicka K, Dobes F |