1 - 14 |
Advanced coatings on high temperature applications Narita T, Izumi T, Nishimoto T, Shibata Y, Thosin KZ, Hayashi S |
15 - 26 |
Metal dusting reaction mechanisms Young DJ |
27 - 36 |
High temperature passive oxidation mechanism of CVD SiC Goto T |
37 - 44 |
Void formation in magnetite scale formed on iron at 823 K - Elucidation by chemical potential distribution Ueda M, Kawamura K, Maruyama T |
45 - 52 |
Transition from external to internal oxidation of single phase binary alloys He YD, Ma J, Li ZW, Gao W |
53 - 60 |
Behaviour of copper and nickel during high temperature oxidation of steel containing them Kondo Y |
61 - 68 |
Modem analytical techniques in high temperature oxidation and corrosion Graham MJ |
69 - 76 |
In situ study of real structure effects on the initial oxidation of FeCrAl alloys by two-dimensional high temperature X-ray diffraction Kodjamanova P, Fietzek H, Juez-Lorenzo M, Kolarik V, Hattendorf H |
77 - 85 |
Oxidation of a low carbon, low silicon steel in air at 600-920 degrees C Chen RY, Yuen WYD |
87 - 92 |
Micro-area analysis of the corrosion products formed on alloy 825 exposed to simulated waste incineration boiler conditions Sato A, Takahashi H, Yoshiba M |
93 - 101 |
Gas-tight oxides - Reality or just a hope Anghel C, Hultquist G, Dong Q, Rundgren J, Saeki I, Limback M |
103 - 110 |
Phase equilibria of the nickel-aluminum-chromium system at 1150 degrees C Kitajima Y, Hayashi S, Narita T |
111 - 118 |
Initial oxidation rate law of binary alloys by hopping migration of cations Ishikawa I, Nanjo H |
119 - 128 |
Current understanding of steam oxidation - Power plant and laboratory experience Saunders SRJ, McCartney LN |
129 - 137 |
The role of alloy composition on the steam oxidation resistance of 9-12%Cr steels Osgerby S, Fry A |
139 - 146 |
Effects of hydrogen on the corrosion resistance of metallic materials and semiconductors Hultquist G, Anghel C, Szakalos P |
147 - 154 |
Beneficial effect of impurity sulfur on high-temperature steam oxidation of high chromium ferritic steels Murata Y, Nakai M, Nagai K, Morinaga M, Sasaki Y, Hashizume R |
155 - 162 |
The effect of gas flow rate on the oxide scale morphology of a 10%Cr-ferritic steels in Ar-H(2)O and Ar-H(2)-H(2)O mixtures Zurek J, Michalik M, Singheiser L, Quadakkers WJ |
163 - 170 |
TDS measurement of hydrogen released from stainless steel oxidized in H(2)O-containing atmospheres Yamauchi A, Yamauchi Y, Hirohata Y, Hino T, Kurokawa K |
171 - 180 |
Effect of chromium content on the oxidation behaviour of high-speed steels under dry and moist air environments Monteiro MJ, Rizzo FC |
181 - 188 |
Steam oxidation of TP 347H FG in power plants Hansson AN, Montgomery M |
189 - 196 |
Hot corrosion and steam oxidation properties of new heat resistant steels for ultra super critical boilers Fukuda Y, Shimizu M |
197 - 203 |
The relationship between high-temperature steam oxidation and hydrogen dissolution in high-chromium ferritic steels Nagai K, Nakai M, Kunieda T, Murata Y, Morinaga M, Matsuda S, Kanno M |
205 - 212 |
Steam oxidation testing of coatings for next generation steam power plant components Aguero A, Gutierrez M, Muelas R |
213 - 219 |
Corrosion rate and oxide scale characteristics of austenitic alloys in supercritical water Watanabe Y, Daigo Y |
221 - 228 |
Oxidation behavior of Pt plus Hf-modified gamma-Ni plus gamma'-Ni(3)Al alloys Izumi T, Gleeson B |
229 - 238 |
Early-stage oxidation behavior of gamma'-Ni(3)Al-based alloys with and without Pt addition Hayashi S, Narita T, Gleeson B |
239 - 246 |
2CaO center dot SiO(2)-CaO center dot ZrO(2) thermal barrier coating formed by plasma spray process Mifune N, Harada Y |
247 - 253 |
Fundamental coating development study to improve the isothermal oxidation resistance and thermal cycle durability of thermal barrier coatings Torigoe T, Oguma H, Okada I, Xu GC, Fujita K, Nakayama A, Maruyama T, Nishio K |
255 - 265 |
Preparation of highly oxidation-resistant surface by molten salt electrodeposition Hara M, Fukumoto M |
267 - 276 |
Strain tolerance and microstructure of thermal barrier coatings produced by electron beam physical vapor deposition process Wada K, Ishiwata Y, Yamaguchi N, Matsubara H |
277 - 284 |
Wet oxidation: A promising way for fabrication of zinc oxide nanostructures Gao W, Li ZW |
285 - 292 |
Interdiffusion between Ni based superalloy and diffusion barrier coatings at 1423K Matsumaru H, Hayashi S, Narita T |
293 - 300 |
Interdiffusion behavior of electroplated platinum-iridium alloys on nickel-base single crystal superalloy TMS-82+ Wu YN, Suzuki A, Murakami H, Kuroda S |
301 - 308 |
Isothermal oxidation of Pt modified and Ru modified aluminide coating on a fourth generation single crystal superalloy Matsuoka Y, Matsunaga Y, Nakagawa K, Taniguchi S |
309 - 316 |
Development of an oxidation resistant coating on Nb-based ultra-high temperature alloy Saito K, Hayashi S, Narita T, Iwanaga I, Tanaka R |
317 - 322 |
Oxidation behavior of Ru-containing Ni-base single-crystal superalloys Kawagishi K, Sato A, Sato A, Kobayashi T, Harada H |
323 - 330 |
Micro-/nano-crystal aluminized ODS coatings Zhan ZL, He YD, Wang DR, Gao W |
331 - 338 |
Novel electrodeposited Ni-based nanocomposite precursors for nitriding and low temperature chromizing Peng X, Zhao J, Zhang H, Wang F |
339 - 344 |
Oxidation property of CoNiCrAlY coatings prepared by various thermal spraying techniques Shibata M, Kuroda S, Watanabe M, Sakamoto Y |
345 - 352 |
In situ observation of failure behavior for plasma sprayed thermal barrier coating systems under static loadings Takahashi S, Yoshiba M, Kawamura R, Harada Y |
353 - 359 |
Environmental effect of hot corrosion on creep and fatigue failure of thermal barrier coating systems Takahashi S, Yoshiba M, Kakuta W, Matsuoka S, Harada Y |
361 - 367 |
Development of new bond coat system in Ni-base alloys Sato A, Harada H, Kawagishi K |
369 - 376 |
Effect of zirconium on cyclic-oxidation of Ni-4OCr-3Re alloys with alpha-Cr/beta-NiAl coatings Shibata Y, Hayashi S, Narita T |
377 - 384 |
Formation of Ni aluminide layer containing La by molten-salt electrodeposition and cyclic-oxidation resistance Fukumoto M, Hara M, Narita T |
385 - 392 |
Effect of laser fusing on hot corrosion resistance of nickel based self fluxing alloy coating Li Y, Nishio K, Katoh M, Yamaguchi T, Okamine S |
393 - 400 |
Mechanical properties and adherence of oxide scales Schutze M, Malessa M, Renusch D, Tortorelli PF, Wright IG, Dooley RB |
401 - 408 |
The effect of oxide scale on the mechanical behavior of low alloyed steel at high temperature Favergeon J, Moulin G, Makni A, Lahoche L |
409 - 415 |
Effect of scale microstructure on scale adhesion of low carbon sheet steel Kobayashi A, Seto K, Urabe T, Yamada K, Sato K |
417 - 424 |
Exfoliation and fracture behavior of oxide films formed on titanium and its alloy in high temperature environments Oka YI, Yamabe T, Tsumura T |
425 - 432 |
Interaction between mechanical loading in creep and reactivity of zirconium and zircaloy in temperature Moulin G, El Tahhan R, Favergeon J, Viennot M, Berger P |
433 - 440 |
Strains in thermally growing alumina films measured in-situ using synchrotron x-rays Hou PY, Paulikas AP, Veal BW |
441 - 449 |
Quantitative adhesion energy values of chromia-rich thermal oxides on stainless steels determined by blister and tensile tests Galerie A, Dupeux M, Wouters Y, Toscan F |
451 - 459 |
The effects of steel composition on the oxidation kinetics, scale structure, and scale-steel interface adherence of low and ultra-low carbon steels Chen RY, Yuen WYD |
461 - 468 |
Deformation and fracture behavior of surface oxide scale on Fe-13Cr alloy in hot-rolling process Hidaka Y, Anraku T, Ohtsuka N |
469 - 476 |
Hardness of oxide scales on Fe-Si alloys at room- and high-temperatures Amano T, Okazaki M, Takezawa Y, Shiino A, Takeda M, Onishi T, Seto K, Ohkubo A, Shishido T |
477 - 488 |
Oxidation behavior and scale properties on the Si containing steels. Takeda M, Onishi T |
489 - 495 |
In situ growth-stress measurement of Cr(2)O(3) scale formed on stainless steels by Raman spectroscopy Kitamura K, Nishiyama Y, Otsuka N, Kudo T |
497 - 504 |
Effect of Cr content and water vapor on fracture behavior of the scales formed on Fe and Fe-Cr alloy Yanagihara K, Renusch D, Rohrig M, Schutze M |
505 - 512 |
Influence of cooling rate and steel composition on the scale failure characteristics during cooling of Si-containing low carbon steels Taniguchi S, Hanamoto Y, Nakata J |
513 - 522 |
Development and application of high Cr-high Si-Fe-Ni alloys to high efficiency waste-to-energy boilers Kawahara Y, Sasaki K, Nakagawa Y |
523 - 530 |
Experiences with Inconel 625 in biomass and waste incineration plants Montgomery M, Biede O, Larsen OH |
531 - 537 |
Hot corrosion monitoring of waste incineration corrosion processes using electrochemical techniques Perez FJ, Nieto J, Trilleros JA, Hierro MP |
539 - 546 |
Corrosivity of KCl(g) at temperatures above its dew point - Initial stages of the high temperature corrosion of alloy Sanicro 28 at 600 degrees C Pettersson C, Svensson JE, Johansson LG |
547 - 554 |
Influence of chlorine, sulphur and water vapor on high temperature corrosion of Fe, Cr, Ni alloys for waste incinerators Moulin G, Weulersse K, Favergeon J |
555 - 562 |
Effect of alloying elements on corrosion resistance of Ni-base cast alloys in waste incineration environments Noguchi M, Matsuoka K, Sakamoto H, Shigeki U, Sawada Y |
563 - 570 |
The influence of sulphur additions on the corrosive environment in a waste-fired CFB boiler Pettersson J, Pettersson C, Folkeson N, Johansson LG, Skog E, Svensson JE |
571 - 580 |
An overview of metal dusting in synthesis gas environments Szakalos P |
581 - 588 |
The role of copper in resisting metal dusting of Ni-base alloys Nishiyama Y, Otsuka N |
589 - 594 |
Numerical analysis and control of gas carburizing under changes in gas compositions Yokoyama Y, Mizukoshi T, Ishigami I, Usui T |
595 - 601 |
Microstructures of SiO(2) scales formed on MoSi(2) Kurokawa K, Goto D, Kuchino J, Yamauchi A, Shibayama T, Takahashi H |
603 - 607 |
Oxidation rate of magnesia-carbon refractory with aluminum additive Sunayama H, Kawahara M |
609 - 616 |
TEM observation of the initial stage oxidation of TiAl based alloys in a simulated combustion atmosphere Yoshihara M, Taniguchi S, Li XY |
617 - 624 |
Influence of the third element on the high temperature oxidation behavior of gamma'-Ni(3)Al alloys Mikuni S, Hayashi S, Narita T |
625 - 632 |
Influence of additional elements on the oxidation behaviour of Nb-Al-Cr base alloys Taniguchi S, Tanaka H, Maeda T |
633 - 640 |
Influence of ion implantation of several elements on oxidation behavior of TiAl Yoshihara M, Taniguchi S, Furumaki D, Aono M |
641 - 647 |
Isothermal oxidation of sintered beta-FeSi(2) in air Nanko M, Chang SH, Matsumaru K, Ishizaki K, Takeda M |
649 - 655 |
High temperature oxidation of TiAl-1.5wt.%Mn-(0,5,10)wt.%Y(2)O(3) alloys Lee DB |
657 - 663 |
Microstructure and oxidation of AI/BN composites fabricated by the pressureless infiltration method Lee DB |
665 - 672 |
Effect of coatings on the creep and oxidation behavior of TiAl alloys at 1173K in air Nishimoto T, Hayashi S, Narita T |