2158 - 2159 |
Introduction to the special topical issue on ultrahigh-temperature polymer-derived ceramics Raj R, Riedel R, Soraru GD |
2160 - 2164 |
Sol-gel-derived silicon-boron oxycarbide glasses containing mixed silicon oxycarbide (SiCxO4-x) and boron oxycarbide (BCYO3-y) units Gervais C, Babonneau F, Dallabonna N, Soraru GD |
2165 - 2169 |
In situ densification behavior in the pyrolysis consolidation of amorphous Si-N-C bulk ceramics from polymer precursors Wan JL, Gasch MJ, Mukherjee AK |
2170 - 2178 |
Crystallization behavior of amorphous silicon carbonitride ceramics derived from organometallic precursors Iwamoto Y, Volger W, Kroke E, Riedel R, Saitou T, Matsunaga K |
2179 - 2183 |
Novel silicon-boron-carbon-nitrogen materials thermally stable up to 2200 degrees C Wang ZC, Aldinger F, Riedel R |
2184 - 2188 |
Precursor-derived Si-B-C-N ceramics: Oxidation kinetics Butchereit E, Nickel KG, Muller A |
2189 - 2196 |
Transmission electron microscopy and electron energy-loss spectroscopy study of nonstoichiometric silicon-carbon-oxygen glasses Turquat C, Kleebe HJ, Gregori G, Walter S, Soraru GD |
2197 - 2202 |
Characterization of oxidized polymer-derived SiBCN fibers Cinibulk MK, Parthasarathy TA |
2203 - 2207 |
Fracture toughness of amorphous precursor-derived ceramics in the silicon-carbon-nitrogen system Bauer A, Christ M, Zimmermann A, Aldinger F |
2208 - 2212 |
Nanoscale densification creep in polymer-derived silicon carbonitrides at 1350 degrees C Shah SR, Raj R |
2213 - 2219 |
Molecular dynamics study of atomic structure and diffusion behavior in amorphous silicon nitride containing boron Matsunaga K, Iwamoto Y |
2220 - 2224 |
Surface damage resistance of gel-derived oxycarbide glasses: Hardness, toughness, and scratchability Rouxel T, Sangleboeuf JC, Guin JP, Keryvin V, Soraru GD |
2225 - 2228 |
Local viscosity of Si-O-C-N nanoscale amorphous phases at ceramic grain boundaries Pezzotti G |
2229 - 2234 |
Transverse thermal conductivity of thin C/SiC composites fabricated by slurry infiltration and pyrolysis Berbon MZ, Dietrich DR, Marshall DB, Hasselman DPH |
2235 - 2239 |
A process for C-f/SiC composites using liquid polymer infiltration Rak ZS |
2240 - 2244 |
Stresses occurring during joining of ceramics using preceramic polymers Lewinsohn CA, Colombo P, Reimanis I, Unal O |
2245 - 2251 |
Mechanical properties of silicon oxycarbide ceramic foams Colombo P, Hellmann JR, Shelleman DL |
2252 - 2255 |
Micro-/macroporous ceramics from preceramic precursors Schmidt H, Koch D, Grathwohl G, Colombo P |
2256 - 2259 |
Electrical characterization of polymethylsiloxane/MoSi2-derived composite ceramics Cordelair J, Greil P |
2260 - 2264 |
Structure and electronic transport properties of Si-(B)-C-N ceramics Hermann AM, Wang YT, Ramakrishnan PA, Balzar D, An LN, Haluschka C, Riedel R |
2265 - 2268 |
Conductive ceramic foams from preceramic polymers Colombo P, Gambaryan-Roisman T, Scheffler M, Buhler P, Greil P |
2269 - 2273 |
Partially reduced cuprous oxide nanoparticles formed in porous glass reaction fields Murase N, Yazawa T |
2274 - 2280 |
Effect of solids loading and dispersant concentration on strain mismatch and deformation of slip-cast green bodies Yates JD, Lombardo SJ |
2281 - 2288 |
In situ neutron powder diffraction study of Ti3SiC2 synthesis Wu ED, Kisi EH, Kennedy SJ, Studer AJ |
2289 - 2295 |
Catalytic and electrochemical properties of doped lanthanum chromites as new anode materials for solid oxide fuel cells Vernoux P, Djurado E, Guillodo M |
2296 - 2302 |
Theoretical investigation of heat transfer in glass forming Viskanta R, Lim JM |
2303 - 2312 |
Formation mechanism of hydrous zirconia particles produced by the hydrolysis of ZrOCl2 solutions: III, kinetics study for the nucleation and crystal-growth processes of primary particles Matsui K, Ohgai M |
2313 - 2317 |
Microwave-hydrothermal synthesis of monodispersed nanophase alpha-Fe2O3 Katsuki H, Komarneni S |
2318 - 2322 |
Hydrothermal treatment of a silica sand complex with lime Watanabe O, Kitamura K, Maenami H, Ishida H |
2323 - 2327 |
Fabrication of lanthanum manganese oxide thin films on yttria-stabilized zirconia substrates by a chemically modified alkoxide method Hwang HJ, Towata A, Awano M |
2328 - 2334 |
Volume fraction and whisker orientation dependence of the electrical properties of SiC-whisker-reinforced mullite composites Gerhardt RA, Ruh R |
2335 - 2342 |
Electrical properties of boron nitride matrix composites: III, observations near the percolation threshold in BN-B4C composites Gerhardt RA, Runyan J, Sana C, McLachlan DS, Ruh R |
2343 - 2350 |
Rheological properties of cement-based extrudates with fibers Li ZJ, Mu B |
2351 - 2355 |
Strength-limiting surface damage in single-crystal sapphire imaged by X-ray topography Black D |
2356 - 2360 |
Ytterbium cation diffusion in yttrium aluminum garnet (YAG) -Implications for creep mechanisms Jimenez-Melendo M, Haneda H, Nozawa H |
2361 - 2365 |
Morphology of vickers indent flaws in soda-lime-silica glass Whittle BR, Hand RJ |
2366 - 2370 |
Low-frequency measurements on the grain-boundary internal friction peak in chlorine-doped silicon nitride Pezzotti G |
2371 - 2376 |
Grain-boundary viscosity of preoxidized and nitrogen-annealed silicon carbides Pezzotti G, Kleebe HJ, Nishimura H, Ota K |
2377 - 2384 |
Effect of flaw state on the strength of brittle coatings on soft substrates Kim HW, Deng Y, Miranda P, Pajares A, Kim DK, Kim HE, Lawn BR |
2385 - 2393 |
Damage evolution and stress analysis in zirconia thermal barrier coatings during cyclic and isothermal oxidation Singh JP, Nair BG, Renusch DP, Sutaria MP, Grimsditch MH |
2394 - 2400 |
Tensile creep behavior of a gas-pressure-sintered silicon nitride containing silicon carbide Krause RF, Wiederhorn SM |
2401 - 2408 |
Unusual elastic and mechanical behaviors of copper phosphate glasses with different copper valence states Miura T, Watanabe T, Benino Y, Komatsu T |
2409 - 2414 |
Structural control of elastic constants of mullite in comparison to sillimanite Hildmann B, Ledbetter H, Kim S, Schneider H |
2415 - 2420 |
Phase equilibria in the Hafnia-Yttria-Lanthana system Andrievskaya ER, Lopato LM |
2421 - 2423 |
Nanocrystalline alpha-Al2O3 using sucrose Das RN, Bandyopadhyay A, Bose S |
2424 - 2426 |
Densification behavior in microwave-sintered silicon nitride at 28 GHz Jones MI, Valecillos MC, Hirao K, Toriyama M |
2427 - 2429 |
Visualization of knoop indentation damage of silicon nitride by plasma etching Kanematsu W, Miyajima T, Sando M |
2430 - 2432 |
Silicon nitride/molybdenum disilicide composite with superior long-term oxidation resistance at 1500 degrees C Klemm H, Schubert C |
2433 - 2435 |
Effect of Neodymium : Yttrium aluminum garnet laser irradiation on crystallization in Li2O-Al2O3-SiO2 glass Lee YS, Kang WH, Kim BI, Song SD |
2436 - 2438 |
Lead zirconate titanate thin films on base-metal foils: An approach for embedded high-permittivity passive components Maria JP, Cheek K, Streiffer S, Kim SH, Dunn G, Kingon A |
2439 - 2441 |
Evidence of nearest-neighbor ordering in wet-processed zirconia-nickel composites Pecharroman C, Lopez-Esteban S, Bartolome JF, Moya JS |
2442 - 2444 |
Separate growth of alpha- and beta-Si3N4 whiskers on or near a carbon substrate by carbothermal reduction Shimada S, Kataoka T |
2445 - 2447 |
Mechanical properties of CoAl materials with the combined additions of ZrO2(3Y) and Al2O3 Takano Y, Yoshinaka M, Hirota K, Yamaguchi O |
2448 - 2450 |
Thermal and electrical properties in plasma-activation-sintered silicon carbide with rare-earth-oxide additives Zhan GD, Mitomo M, Xie RJ, Mukherjee AK |
2451 - 2453 |
Experimental observations of high fracture resistance in silicon carbide/alumina laminated composites Krishnamurthy R, Sheldon BW |
2454 - 2456 |
Direct evidence for low-density regions in compacted spray-dried powders Saito Y, Tanaka S, Uchida N, Uematsu K |